Polymer Property : Molecular Weight = 2900 g/mol Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Molecular Weight 2900 g/mol
2900 g/mol
Solvay Specialty Polymers FOMBLIN® LC200 PFPE Lubricant
FOMBLIN LC perfluoropolyether fluids have the following unique features: excellent wear characteristics; very good low temperature properties; cost-effective; and outstanding for applications requir..
Molecular Weight 2900 g/mol
2900 g/mol
Mw; ETM 300-83
ExxonMobil ESCOREZ™ 1102 (Americas) Petroleum Hydrocarbon Resin
Aliphatic hydrocarbon resin which is designed for use in a varity of applicaitons.Availability: Central America, North America and South AmericaInformation provided by ExxonMobil Chemical
Molecular Weight 2900 g/mol
2900 g/mol
Mitsui EXCEREX™ 30200B(T) Polymer Processing Aid
EXCEREX™ is an innovative processing improvement agent created with metallocene catalysis technology. EXCEREX™ gains in a number of ares simultaneously, including faster processing speeds, lower ..