Physical Properties | Metric | English | Comments |
---|---|---|---|
Molecular Weight | 290 g/mol | 290 g/mol | |
Dow PAPI™ 901 Polymeric MDI PAPI™ 901 polymeric MDI is a polymethylene polyphenylisocyanate that contains MDI. This product has a high functionality and a high viscosity resulting in highly rigid foams. This product is desi.. |
|||
Molecular Weight | 290 g/mol | 290 g/mol | |
Dow PAPI™ 94 Polymeric MDI PAPI™ 901 polymeric MDI is a polymethylene polyphenylisocyanate that contains MDI. This products low viscosity, low functionality, increased diphenylmethane diisocyanate content and increased perc.. |