Physical Properties | Metric | English | Comments |
---|---|---|---|
Molecular Weight | 286.324 g/mol | 286.324 g/mol | |
Esstech X-943-7422 Triethyleneglycol Dimethacrylate, C14H22O6 Triethylene glycol dimethacrylate is a difunctional monomer that has been the foundation of many long-standing dental formulations. It has ideal water absorptivity and stability properties. Listed .. |
|||
Molecular Weight | 286.324 g/mol | 286.324 g/mol | |
Esstech X-943-7424 Triethyleneglycol Dimethacrylate, C14H22O6 Triethylene glycol dimethacrylate is a difunctional monomer that has been the foundation of many long-standing dental formulations. It has ideal water absorptivity and stability properties. Listed .. |
|||
Molecular Weight | 286.324 g/mol | 286.324 g/mol | |
Esstech X-943-7446 Triethyleneglycol Dimethacrylate, C14H22O6 Triethylene glycol dimethacrylate is a difunctional monomer that has been the foundation of many long-standing dental formulations. It has ideal water absorptivity and stability properties. Listed .. |
|||
Molecular Weight | 286.324 g/mol | 286.324 g/mol | |
Esstech X-943-7466 Triethyleneglycol Dimethacrylate, C14H22O6 Triethylene glycol dimethacrylate is a difunctional monomer that has been the foundation of many long-standing dental formulations. It has ideal water absorptivity and stability properties. Listed .. |