Physical Properties | Metric | English | Comments |
---|---|---|---|
Molecular Weight | 2700 g/mol | 2700 g/mol | |
Solvay Specialty Polymers FOMBLIN® Y L-VAC 16/6 PFPE Pump Oil FOMBLIN Y fluids are a mixture of fluorinated polymers obtained by a photochemical process that begins with hexafluoropropylene. Since the FOMBLIN chemical chain contains only carbon, fluorine, and.. |
|||
Molecular Weight | 2700 g/mol | 2700 g/mol | |
Solvay RHODOLINE® 286N Surfactant Description: Hydrophilic copolymer dispersant. Semi gloss to high gloss, TiO2 slurry, interior/exterior, low foam.Identification: AMMONIUM POLYACRYLATE COPOLYMER SOLUTIONAvailable in: North AmericaA.. |
|||
Molecular Weight | 2700 g/mol | 2700 g/mol | Mw; ETM 300-83 |
ExxonMobil ESCOREZ™ 1315 Petroleum Hydrocarbon Resin Premium aliphatic resin with a high softening point. It is a tackifying resin designed to provide high temperature performance and cohesive strength with a variety of adhesive polymers including me.. |