Physical Properties | Metric | English | Comments |
---|---|---|---|
Molecular Weight | 1700 g/mol | 1700 g/mol | |
Solvay Specialty Polymers FOMBLIN® LC55 PFPE Lubricant FOMBLIN LC perfluoropolyether fluids have the following unique features: excellent wear characteristics; very good low temperature properties; cost-effective; and outstanding for applications requir.. |
|||
Molecular Weight | 1700 g/mol | 1700 g/mol | osmometric |
BASF Luwax® OA 2 Pastilles Description: Hard, emulsifiable polyethylene wax. Used to produce finely dispersed wax emulsions or polishes and many other products. Lubricant for processing PVC.Information provided by BASF |