Physical Properties | Metric | English | Comments |
---|---|---|---|
Molecular Weight | 138000 - 162000 g/mol | 138000 - 162000 g/mol | Triblock |
Kraton® D1192 A (SBS) Liner Block Copolymer Description: Kraton D1192 A is a clear linear block copolymer based on styrene and butadiene with bound styrene of 30% mass. It is supplied from Europe in the physical forms described: Kraton D1192 .. |
|||
Molecular Weight | 138000 - 162000 g/mol | 138000 - 162000 g/mol | Triblock |
Kraton® D1192 B (SBS) Liner Block Copolymer Description: Kraton D1192 B is a clear linear block copolymer based on styrene and butadiene with bound styrene of 30% mass. It is supplied from South America in the physical form described: Kraton .. |
|||
Molecular Weight | 138000 - 162000 g/mol | 138000 - 162000 g/mol | Triblock |
Kraton® D1192 E (SBS) Liner Block Copolymer Description: Kraton D1192 E is a clear linear block copolymer based on styrene and butadiene with bound styrene of 30% mass. It is supplied from Europe in the physical forms described: Kraton D1192 .. |