Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Molecular Weight = 1.50e+6 g/mol Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Molecular Weight 900000 - 1.50e+6 g/mol
900000 - 1.50e+6 g/mol
Lucite International Colacryl ® D120 Acrylic Dental Resin
A range of Methyl Methacrylate polymers designed for use as standard heat-curing denture base resins.Features: Fine free-flowing bead polymers containing residual peroxide initiator; Curing cycles f..
Molecular Weight 900000 - 1.50e+6 g/mol
900000 - 1.50e+6 g/mol
Lucite International Colacryl ® D150 Acrylic Dental Resin
A range of Methyl Methacrylate polymers designed for use as standard heat-curing denture base resins.Features: Fine free-flowing bead polymers containing residual peroxide initiator; Curing cycles f..
Molecular Weight 900000 - 1.50e+6 g/mol
900000 - 1.50e+6 g/mol
Lucite International Colacryl ® D60 Acrylic Dental Resin
A range of Methyl Methacrylate polymers designed for use as standard heat-curing denture base resins.Features: Fine free-flowing bead polymers containing residual peroxide initiator; Curing cycles f..
Molecular Weight 900000 - 1.50e+6 g/mol
900000 - 1.50e+6 g/mol
Lucite International Colacryl ® D80 Acrylic Dental Resin
A range of Methyl Methacrylate polymers designed for use as standard heat-curing denture base resins.Features: Fine free-flowing bead polymers containing residual peroxide initiator; Curing cycles f..
Molecular Weight 900000 - 1.50e+6 g/mol
900000 - 1.50e+6 g/mol
Lucite International Colacryl ® PD12 Acrylic Dental Resin
Methyl Methacrylate polymers and copolymers designed for use as fast heat curing denture base resins.Colacryl denture base resins feature fast polymerisation and a wide choice of process properties...
Molecular Weight 900000 - 1.50e+6 g/mol
900000 - 1.50e+6 g/mol
Lucite International Colacryl ® PD2 Acrylic Dental Resin
A range of Methyl Methacrylate polymers designed for use as standard heat-curing denture base resins.Features: Fine free-flowing bead polymers containing residual peroxide initiator; Curing cycles f..
Molecular Weight 900000 - 1.50e+6 g/mol
900000 - 1.50e+6 g/mol
Lucite International Colacryl ® TS 1649 Acrylic Orthodontic Polymer
A range of methacrylate based copolymers designed for the manufacture of high quality orthodontic dental resins.Features: Excellent dry flow characteristics; Closely controlled particle size; Contai..
Molecular Weight 900000 - 1.50e+6 g/mol
900000 - 1.50e+6 g/mol
Lucite International Colacryl ® TS 1672 Acrylic Orthodontic Polymer
A range of methacrylate based copolymers designed for the manufacture of high quality orthodontic dental resins.Features: Excellent dry flow characteristics; Closely controlled particle size; Contai..
Molecular Weight 900000 - 1.50e+6 g/mol
900000 - 1.50e+6 g/mol
Lucite International Colacryl ® TS1785 Acrylic Dental Resin
Cold-curing denture repair resin with Methyl Methacrylate based copolymers. Features fast polymerisation, easy mixing, good clarity, short hydroflask cure cycles, and excellent pigment acceptance.I..
Molecular Weight 900000 - 1.50e+6 g/mol
900000 - 1.50e+6 g/mol
Lucite International Colacryl ® PD11SG Acrylic Dental Resin
Methyl Methacrylate polymers and copolymers designed for use as fast heat curing denture base resins.Colacryl denture base resins feature fast polymerisation and a wide choice of process properties...
Copyright © lookpolymers.com All Rights Reserved