Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Surface Area | 3.5 m²/g | 3.5 m²/g | |
Omya HYDROCARB® PG-3 Calcium Carbonate A ground calcium carbonate for paper and board coating.Information supplied by Omya North America. |
|||
Specific Surface Area | 3.5 m²/g | 3.5 m²/g | BET |
Nabaltec APYRAL® 40 VS1 Al(OH)3 The high quality and performance of our surface treated APYRAL® 40VS1 and APYRAL® 60VS1 powders complete the APRYAL® product range for highly specialized applications. Examples include, excellent.. |
|||
Specific Surface Area | 3.5 - 7.5 m²/g | 3.5 - 7.5 m²/g | |
Sinotek Materials ZSG-15 Spherical Graphite Also called "Potato Graphite", Spherical Graphite is ideal cathode material for lithium ion batteries. Using high quality natural flake graphite as raw material, a series of shaping, classification.. |
|||
Specific Surface Area | 3.5 - 7.5 m²/g | 3.5 - 7.5 m²/g | |
Sinotek Materials ZSG-23 Spherical Graphite Also called "Potato Graphite", Spherical Graphite is ideal cathode material for lithium ion batteries. Using high quality natural flake graphite as raw material, a series of shaping, classification.. |
|||
Specific Surface Area | 3.5 - 7.5 m²/g | 3.5 - 7.5 m²/g | |
Sinotek Materials ZSG-12 Spherical Graphite Also called "Potato Graphite", Spherical Graphite is ideal cathode material for lithium ion batteries. Using high quality natural flake graphite as raw material, a series of shaping, classification.. |
|||
Specific Surface Area | 3.5 - 7.5 m²/g | 3.5 - 7.5 m²/g | |
Sinotek Materials ZSG-17 Spherical Graphite Also called "Potato Graphite", Spherical Graphite is ideal cathode material for lithium ion batteries. Using high quality natural flake graphite as raw material, a series of shaping, classification.. |
|||
Specific Surface Area | 3.5 - 7.5 m²/g | 3.5 - 7.5 m²/g | |
Sinotek Materials ZSG-20 Spherical Graphite Also called "Potato Graphite", Spherical Graphite is ideal cathode material for lithium ion batteries. Using high quality natural flake graphite as raw material, a series of shaping, classification.. |
|||
Specific Surface Area | 3.5 m²/g | 3.5 m²/g | Size E |
Vesta Ceramics SicoMill® Grade 2 Silicon Powder General Description:SicoMill® is a fine-grained silicon powder, specially developed for the ceramic industry. We have five standard grinding grades, but we can produce powders adapted to single cu.. |
|||
Specific Surface Area | 3.5 m²/g | 3.5 m²/g | Size E |
Vesta Ceramics SicoMill® Grade 4 Silicon Powder General Description:SicoMill® is a fine-grained silicon powder, specially developed for the ceramic industry. We have five standard grinding grades, but we can produce powders adapted to single cu.. |
|||
Specific Surface Area | 3.5 m²/g | 3.5 m²/g | BET |
Nabaltec APYRAL® 40CD Al(OH)3 APYRAL ® from Nabaltec is an environmentally friendly halogen free product which is used as a flame retardant filler in a wide variety of rubber and polymeric materials. During thermal decompositio.. |
|||
Specific Surface Area | 3.5 - 7.5 m²/g | 3.5 - 7.5 m²/g | |
Sinotek Materials ZSG-25 Spherical Graphite Also called "Potato Graphite", Spherical Graphite is ideal cathode material for lithium ion batteries. Using high quality natural flake graphite as raw material, a series of shaping, classification.. |