Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Specific Surface Area = 25 m²/g Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Specific Surface Area 25 m²/g
25 m²/g
NanoAmor 95%; OD: 200-500 nm Carbon Nanofibers
ApplicationsCatalyst support materialsElectronic devicesFiber/polymer nanocomposites for enhanced electrical conductivityFiber/polymer nanocomposites for enhanced strengthFuel-cell electrodesGas sto..
Specific Surface Area 25 - 35 m²/g
25 - 35 m²/g
BET
NanoAmor 95%; OD: 80-200 nm Carbon Nanofibers
ApplicationsCatalyst support materialsElectronic devicesFiber/polymer nanocomposites for enhanced electrical conductivityFiber/polymer nanocomposites for enhanced strengthFuel-cell electrodesGas sto..
Specific Surface Area 25 - 35 m²/g
25 - 35 m²/g
BET
NanoAmor 99.8%; OD: 80-200 nm Graphitized Carbon Nanofibers
ApplicationsCatalyst support materialsElectronic devicesFiber/polymer nanocomposites for enhanced electrical conductivityFiber/polymer nanocomposites for enhanced strengthFuel-cell electrodesGas sto..
Specific Surface Area 25 - 35 m²/g
25 - 35 m²/g
Zircar Zirconia ZYP-30 Zirconia Powder
Zircar Zirconia Powder Type ZYP is an ultra fine, highly reactive powder composed of yttria- stabilized zirconia. It is offered with two different surface areas; Type ZYP-30 has a surface area of 25..
Specific Surface Area 25 m²/g
25 m²/g
BET Analysis
Gwent Electronic Materials P2121112P1 Acid Vapor Plasma Modified Graphene Nanoplatelets
Production Method: Plasma Exfoliation of Natural GraphiteColor: Black/Grey Trial product which has not yet been extensively tested.Information provided by Gwent Electronic Materials Ltd.
Specific Surface Area 25 m²/g
25 m²/g
BET Analysis
Gwent Electronic Materials P2121112P2 Argon Plasma Modified Graphene Nanoplatelets
Production Method: Plasma Exfoliation of Natural GraphiteColor: Black/Grey Trial product which has not yet been extensively tested.Information provided by Gwent Electronic Materials Ltd.
Specific Surface Area 25 m²/g
25 m²/g
BET Analysis
Gwent Electronic Materials P2121112P4 Nitrogen Plasma Modified Graphene Nanoplatelets
Production Method: Plasma Exfoliation of Natural GraphiteColor: Black/Grey Trial product which has not yet been extensively tested.Information provided by Gwent Electronic Materials Ltd.
Specific Surface Area 25 m²/g
25 m²/g
BET Analysis
Gwent Electronic Materials P2121112P5 Ammonia Plasma Modified Graphene Nanoplatelets
Production Method: Plasma Exfoliation of Natural GraphiteColor: Black/Grey Trial product which has not yet been extensively tested.Information provided by Gwent Electronic Materials Ltd.
Specific Surface Area 25 m²/g
25 m²/g
BET Analysis
Gwent Electronic Materials P2121112P6 Oxygen Plasma Modified Graphene Nanoplatelets
Production Method: Plasma Exfoliation of Natural GraphiteColor: Black/Grey Trial product which has not yet been extensively tested.Information provided by Gwent Electronic Materials Ltd.
Specific Surface Area 25 m²/g
25 m²/g
BET Analysis
Gwent Electronic Materials P2121112P3 Tetrafluoromethane Plasma Modified Graphene Nanoplatelets
Production Method: Plasma Exfoliation of Natural GraphiteColor: Black/Grey Trial product which has not yet been extensively tested.Information provided by Gwent Electronic Materials Ltd.
Specific Surface Area 25 - 35 m²/g
25 - 35 m²/g
Zircar Zirconia ZYP-30 Zirconia Powder
Zircar Zirconia Powder Type ZYP is an ultra fine, highly reactive powder composed of yttria- stabilized zirconia. It is offered with two different surface areas; Type ZYP-30 has a surface area of 25..
Specific Surface Area 25 - 50 m²/g
25 - 50 m²/g
American Elements Hafnium Oxide Nanopowder
General DescriptionHafnium Oxide or Hafnia Nanopowder or Nanoparticles (HfO), nanodots or nanocrystals are white high surface area particles. Nanoscale Hafnium Oxide Nanoparticles are typically 5 - ..
Specific Surface Area 25 - 50 m²/g
25 - 50 m²/g
American Elements Indium Oxide Nanopowder
General DescriptionIndium Oxide Nanopowder or Nanoparticles (InO), nanodots or nanocrystals are white high surface area particles. Nanoscale Indium Oxide Nanoparticles are typically 5 - 100 nanomete..
Specific Surface Area 25 - 50 m²/g
25 - 50 m²/g
American Elements Magnesium Oxide Nanopowder
General DescriptionMagnesium Oxide Nanoparticles or Magnesia Nanoparticles (MgO) Nanoparticles, nanodots or nanopowder are spinel, high surface area particles. Nanoscale Magnesium Oxide Nanoparticle..
Specific Surface Area 25 - 50 m²/g
25 - 50 m²/g
American Elements Manganese Oxide Nanopowder
General DescriptionManganese Oxide Nanopowder (MnO), nanodots or nanoparticles are high surface area particles. Nanoscale Manganese Oxide Nanoparticles are typically 5 - 100 nanometers (nm) with spe..
Specific Surface Area 25 - 50 m²/g
25 - 50 m²/g
American Elements Niobium Oxide Nanoparticles
General DescriptionNiobium Oxide ( MoO) Nanopowder or Nanoparticles, nanodots or nanocrystals are ferric and ferrous spherical or faceted high surface area oxide magnetic nanostructure particles. Na..
Specific Surface Area 25 - 75 m²/g
25 - 75 m²/g
American Elements Silicon Nitride Nanoparticles
General DescriptionSilicon Nitride (SiN) Nanoparticles, nanodots or nanopowder are spherical high surface area particles. Nanoscale Silicon Nitride Particles are typically 10 - 100 nanometers (nm) w..
Specific Surface Area 25 - 50 m²/g
25 - 50 m²/g
American Elements Silicon Oxide Nanopowder
General DescriptionSilicon Oxide (SiO2) Nanopowder, Silica Nanoparticles or nanodots are high surface area particles. Nanoscale Silicon Oxide Nanoparticles or Silica Particles are typically 5 - 100 ..
Specific Surface Area 25 - 50 m²/g
25 - 50 m²/g
American Elements Yttria stabilized Zirconia
General DescriptionYttria stabilized Zirconia or Zirconium Oxide Nanopowder or Nanoparticles (YSZ), nanodots or nanocrystals are white high surface area particles available fully stabilized (8 mol%)..
Specific Surface Area 25 - 50 m²/g
25 - 50 m²/g
American Elements Zirconium Oxide Nanopowder
General DescriptionZirconium Oxide or Zirconia Nanopowder or Nanoparticles (ZrO2), nanodots or nanocrystals are white high surface area particles available in monoclinic or as stabilized or doped wi..
Specific Surface Area 25 m²/g
25 m²/g
BASF Paliotol™ Yellow L 2140 Color Additive
Description: Isoindoline yellow with high opacity and reddish shade for OEM and industrial coatings.Suitable for: Baking systems, Waterborn systems, Acrylic-isocyanate systems, Acid curing system, A..
Copyright © lookpolymers.com All Rights Reserved