Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Surface Area | 15 m²/g | 15 m²/g | BET |
Nabaltec APYRAL® 200 SM Al(OH)3 APYRAL ® from Nabaltec is an environmentally friendly halogen free product which is used as a flame retardant filler in a wide variety of rubber and polymeric materials. During thermal decompositio.. |
|||
Specific Surface Area | 15 - 45 m²/g | 15 - 45 m²/g | BET |
Magyar Aluminum ALO-Ex31 Alumina Calcined Alumina |
|||
Specific Surface Area | 15 m²/g | 15 m²/g | |
Momentive Performance Materials AC6041 Boron Nitride (BN) Powder Crystalline hexagonal platelet morphology. AC6041 shows good dispersion, with enhanced lubricity and thermal properties. AC6041 powder is readily used in the production of many advanced materials... |
|||
Specific Surface Area | 15 m²/g | 15 m²/g | |
Momentive Performance Materials PolarTherm® PT132 Boron Nitride (BN) Powder Boron Nitride powders are produced by GE Advanced Ceramics in more than 50 individual (standard and custom) grades to meet a wide variety of application needs.For use in: Electrically insulating/the.. |
|||
Specific Surface Area | 15 - 20 m²/g | 15 - 20 m²/g | BET |
H.C. Starck Grade HD 15 Boron Carbide, B4C Powder for sintering.Abrasive grit or powder (grinding, lapping, polishing)Wear resistant engineering components (e.g. sand-blasting and water jet nozzlesLight weight ceramic armorMetal infiltration.. |
|||
Specific Surface Area | 15 - 20 m²/g | 15 - 20 m²/g | BET |
H.C. Starck Grade HS Boron Carbide, B4C Powder for sintering.Abrasive grit or powder (grinding, lapping, polishing)Wear resistant engineering components (e.g. sand-blasting and water jet nozzlesLight weight ceramic armorMetal infiltration.. |
|||
Specific Surface Area | >= 15 m²/g | >= 15 m²/g | BET |
H.C. Starck high purity Aluminum Magnesium Spinel Single phase Mg-Al-SpinelSintering additive for Si3N4Starting powder for spinel-type electro-ceramics |
|||
Specific Surface Area | 15 - 20 m²/g | 15 - 20 m²/g | |
American Elements Titanium Nanoparticles General DescriptionTitanium (Ti) Nanoparticles, nanodots or nanopowder are spherical or faceted high surface area metal particles. Nanoscale Titanium Particles are typically 10 - 80 nanometers (nm) .. |
|||
Specific Surface Area | 15 - 45 m²/g | 15 - 45 m²/g | |
American Elements Z-MITE™ Zinc Oxide Nanopowder General DescriptionZ-MITE powders are inorganic zinc-oxide nanoparticles with antibacterial, antifungal, anti-corrosion, catalytic, and UV filtering properties. Z-MITE-A products are uncoated and hy.. |
|||
Specific Surface Area | 15 - 50 m²/g | 15 - 50 m²/g | |
American Elements Calcium Oxide Nanopowder General DescriptionCalcium Oxide ( CaO) Nanopowder or Nanoparticles, nanodots or nanocrystals are ferric and ferrous spherical or faceted high surface area oxide magnetic nanostructure particles. Na.. |
|||
Specific Surface Area | 15 m²/g | 15 m²/g | |
BASF Paliotol™ Yellow L 0962 Color Additive Description: Opaque quinophthalone yellow with excellent rheologySuitable for: Baking systems, Waterborn systems, Acrylic-isocyanate systems, Acid curing system and Airdrying systemsInformation prov.. |
|||
Specific Surface Area | 15 - 21 m²/g | 15 - 21 m²/g | |
Momentive Performance Materials PolarTherm® PT180 Boron Nitride (BN) Powder Fine Hexagonal BN PowderWhen used in a variety of polymeric materials, PolarTherm™'s heat dissipating capability helps extend the service life and enhance the reliability of electronic componen.. |