Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Particle Size = 80 µm Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Particle Size <= 80 µm
<= 80 µm
90% smaller than
Nyco NYGLOS® M20 Wollastonite
Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctive particle morphology makes wollastonite an ideal performance mineral for a br..
Particle Size 80 - 120 µm
80 - 120 µm
Median Grain Diameter
Nabaltec GRANALOX® NM 9620 F Ceramic Bodies
Nabaltec`s GRANALOX® Ceramic bodies are produced under rigid quality control of green and sintered density, shrinkage, porosity, loss on ignition and granulate size. The properties of the corundum ..
Particle Size 80 - 120 µm
80 - 120 µm
Mean Granulate Size
Nabaltec GRANALOX® NM 9916 F Ceramic Body
Nabaltec's GRANALOX® Ceramic bodies are produced under rigid quality control of green and sintered density, shrinkage, porosity, loss on ignition and granulate size. The properties of the corundum ..
Particle Size 80 µm
80 µm
Mean
Potters Industries Q-Cel® 7019 Hollow Engineered Glass Microspheres
Q-CEL® hollow glass microspheres are alternatives to conventional fillers and additives such as silicas, calcium carbonates, talc, clay, etc. A variety of particle sizes, densities and strengths me..
Particle Size 80 µm
80 µm
Method C; ASTM D1921
Solvay Specialty Polymers Halar® 6014 Polyethylene, Chlorotrifluoroethylene (ECTFE)  (Unverified Data**)&l
Halar® 6014 is a clear, semi-crystalline melt processable fluorinated resin. It is designed for electrostatic powder coatings and is particularly recommended for use as a topcoat in protection and ..
Particle Size 80 µm
80 µm
Method C; ASTM D1921
Solvay Specialty Polymers Halar® 6014F Polyethylene, Chlorotrifluoroethylene (ECTFE)  (Unverified Data**)&
Halar® 6014F is a clear, semi-crystalline melt processable fluorinated resin. It is designed for electrostatic powder coatings and is particularly recommended for use as a topcoat in protection and..
Particle Size 80 µm
80 µm
Method C; ASTM D1921
Solvay Specialty Polymers Halar® 6914 Polyethylene, Chlorotrifluoroethylene (ECTFE)  (Unverified Data**)&l
Halar® 6914 is a gray, semi-crystalline melt processable fluorinated primer. It is designed to be applied directly to substrates by electrostatic or fluidized bed techniques. In particular Halar® ..
Particle Size 80 µm
80 µm
Gromax EP-5016M Unplasticized Vinyl Acetate homopolymer
Product Description: EP-5016M is a water redispersible vinyl acetate homopolymer powder that is readily dispersible in water and forms stable emulsion. This redispersible powder is especially recomm..
Particle Size 80 - 100 µm
80 - 100 µm
Lucite International Colacryl ® DP300 Specialty Acrylic Resin
This is a high molecular weight PMMA resin. PMMA resins are characterised by high physical strength and abrasion resistance.Applications:This resin is used in the production of porous polymer molds ..
Particle Size 80 - 100 µm
80 - 100 µm
Lucite International Colacryl ® DP300S Acrylic Dental Resin
Methyl Methacrylate polymers and copolymers designed for use as fast heat curing denture base resins.Colacryl denture base resins feature fast polymerisation and a wide choice of process properties...
Particle Size 80 - 100 µm
80 - 100 µm
Lucite International Colacryl ® DP300S Specialty Acrylic Resin
Colacryl® DP 300S has been designed for use as a dental polymer. Typical applications for this product include formulated, acrylic tooth polymer for manufacture of artificial teeth and denture ba..
Particle Size <= 80 µm
<= 80 µm
> 99 wt.%; DIN EN ISO 4610
Suzhou Hipro Polymers Hiprolon® 11 PES Colorized Nylon powder
Hiprolon® 11 PES colorized electrostatic polyamide powder is partly comprised of bio-renewable raw materials. It has excellent weather ability, chemical resistance, wear resistance, impact resist..
Particle Size <= 80 µm
<= 80 µm
> 99 wt.%; DIN EN ISO 4610
Suzhou Hipro Polymers Hiprolon® 211 PES Colorized Nylon powder
Hiprolon® 211 PES colorized electrostatic polyamide powder is fully comprised of bio-renewable raw materials. It has excellent weather ability, chemical resistance, wear resistance, impact resist..
Particle Size 80 µm
80 µm
TIMCAL TIMREX® M80 mesh FR Natural Flake Graphite
TIMREX Natural Flake Graphite is produced in a wide range of products distinguished by particle size distribution, chemistry and carbon content. Timcal mines the graphite from its own source in Lac-..
Particle Size 80 µm
80 µm
at a density of 1.48 g/cc, pressure of 2.5 t/cc
TIMCAL TIMREX® T44 Primary Synthetic Graphite
TIMREX Primary Synthetic Graphite is produced in a unique highly controlled graphitization process which assures narrow specifications and unequalled consistent quality due to: monitoring of all pro..
Particle Size <= 80 µm
<= 80 µm
Top Size
Excalibar NewBar™ API Barite BaSO4 Powder
NewBar™ API barite product is manufactured from a high-quality natural barium sulfate ore. Strict quality control results in a consistent product that is used in all phases of oil and gas explorati..
Particle Size <= 80 µm
<= 80 µm
Top Size
Excalibar NewWate™ Barite BaSO4 Powder
NewWate™ barite is manufactured from a high-quality natural barium sulfate ore. Strict quality control results in a consistent product that is used in all phases of oil and gas exploration. NewWate..
Particle Size 80 µm
80 µm
90th%
3M K37 Glass Bubbles
3M™ Glass Bubbles are engineered hollow glass microspheres that are alternatives to conventional fillers and additives such as silicas, calcium carbonate, talc, clay, etc., for many demanding appli..
Particle Size 80 µm
80 µm
Effective Top Size
3M K46 Glass Bubbles
3M™ Glass Bubbles are engineered hollow glass microspheres that are alternatives to conventional fillers and additives such as silicas, calcium carbonate, talc, clay, etc., for many demanding appli..
Particle Size 80 µm
80 µm
Effective Top Size
3M S32 Glass Bubbles
3M™ Glass Bubbles are engineered hollow glass microspheres that are alternatives to conventional fillers and additives such as silicas, calcium carbonate, talc, clay, etc., for many demanding appli..
Particle Size 80 µm
80 µm
Effective Top Size
3M S35 Glass Bubbles
3M™ Glass Bubbles are engineered hollow glass microspheres that are alternatives to conventional fillers and additives such as silicas, calcium carbonate, talc, clay, etc., for many demanding appli..
Particle Size <= 80 µm
<= 80 µm
90% smaller than
Nyco ULTRAFIBRE® M20 Wollastonite
Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctive particle morphology makes wollastonite an ideal performance mineral for a br..
Particle Size 80 µm
80 µm
95th%
3M D32/4500 Glass Bubbles
3M™ Glass Bubbles are engineered hollow glass microspheres that are alternatives to conventional fillers and additives such as silicas, calcium carbonate, talc, clay, etc., for many demanding appli..
Particle Size 80 µm
80 µm
Method C; ASTM D1921
Solvay Specialty Polymers Halar® 6514 Polyethylene, Chlorotrifluoroethylene (ECTFE)  (Unverified Data**)&l
Halar 6514 is a black, semi-crystalline melt processable fluorinated primer. It is designed to be applied directly to substrates by electrostatic or fluidized bed techniques. In particular Halar 651..
Particle Size 80 µm
80 µm
Method C; ASTM D1921
Solvay Specialty Polymers Halar® 6614 Polyethylene, Chlorotrifluoroethylene (ECTFE)  (Unverified Data**)&l
Halar® 6614 is a green, semi-crystalline melt processable fluorinated primer. It is designed to be applied directly to substrates by electrostatic or fluidized bed techniques. In particular Halar®..
Particle Size 80 µm
80 µm
Before Conversion
Silberline Sparkle Silvet® 764-30-E1
Sparkle Silvet® E1 grades are easy to disperse and are compatible with a variety of polymers, particularly polyolefins. They are typically used to make concentrates or compounds for use in final pr..
Copyright © lookpolymers.com All Rights Reserved