Physical Properties Metric English Comments
Particle Size 690 µm
690 µm
Asahi Glass Fluon® PA1025Z 25% Glass Fiber, PTFE Filled Compound
Fluon®PTFE FC has improved creep and wear resistance. A wide range of fillers such as glass fiber, graphite, bronze, carbon fiber are available. Information provided by Asahi Glass Company, Inc.