Physical Properties | Metric | English | Comments |
---|---|---|---|
Particle Size | 650 - 900 µm | 650 - 900 µm | Mean particle size |
Solvay Chemicals Oxyper® S142 Sodium Percarbonate Oxyper® S142 is a stabilized grade of sodium percarbonate (Sodium carbonate peroxyhydrate) specially designed for use in formulated bleach additive products, detergent powders and tablets, automa.. |
|||
Particle Size | 650 - 950 µm | 650 - 950 µm | Mean particle size |
Solvay Chemicals Oxyper® SHC Sodium Percarbonate Oxyper® SHC is a high coated, stabilized grade of sodium percarbonate (Sodium carbonate peroxyhydrate) specially designed for use in bleach additive products, detergent powders and tablets, autom.. |
|||
Particle Size | 650 µm | 650 µm | ASTM D4894 |
Daikin POLYFLON M-391 PTFE Molding Powder, Free Flow Free flow powder.Processing Methods: Compression molding and automatic or semi-automatic compression molding.Features: Used if concerned about insufficient molding pressure for flat sheets.Informati.. |
|||
Particle Size | 650 µm | 650 µm | |
Asahi Glass Fluon® G307 PTFE Granular Powder Fluon®PTFE granular powders (molding powders) are used for the production of sheets, rods, billets and other general moldings.Information provided by Asahi Glass Company, Inc. |