Physical Properties | Metric | English | Comments |
---|---|---|---|
Particle Size | 600 - 850 µm | 600 - 850 µm | |
Potters Industries A-Series P-0337 Soda-Lime Silica Technical Quality Solid Glass Spheres Technical Quality, A-Series glass spheres are used to reduce particle size in coatings and inks. Glass Spheres used in oil well drilling improve lubrication and overall efficiencies of down hole oil.. |
|||
Particle Size | 600 - 1000 µm | 600 - 1000 µm | |
Polimeri Europa Extir® Verdi VR A3000 AE Expandable Polystyrene - Flame Retardant Product Description:Extir Verdi VR A3000 AE is a flame-retardant expandable polystyrene in the form of spherical beads of medium particle size, containing pentane as blowing agent.Extir does not con.. |
|||
Particle Size | 600 - 1000 µm | 600 - 1000 µm | |
Polimeri Europa Extir® D 3000 AE Expandable Polystyrene - Flame Retardant Product Description:Extir D 3000 AE is a flame-retardant expandable polystyrene in the form of spherical beads of medium particle size, containing pentane as blowing agent.Extir does not contain CFC.. |
|||
Particle Size | 600 - 1100 µm | 600 - 1100 µm | |
Polimeri Europa Extir® EH 3000 Expandable Polystyrene Extir EH 3000 is an expandable polystyrene in the form of spherical beads of medium particle size, with a low pentane content as blowing agent. Extir does not contain CFC or HCFC. Extir EH 3000 is u.. |
|||
Particle Size | 600 - 1000 µm | 600 - 1000 µm | |
Polimeri Europa Extir® GEO 3000 AE Expandable Polystyrene - Flame Retardant Product Description:Extir GEO 3000 AE is a flame-retardant expandable polystyrene in the form of spherical beads of medium particle size, containing pentane as blowing agent.Extir does not contain C.. |
|||
Particle Size | 600 - 1000 µm | 600 - 1000 µm | |
Polimeri Europa Extir Leonardo A 3000 AE Expandable Polystyrene
(discontinued **) Extir A 3000 AE is a flame retardant expandable polystyrene in the form of spherical beads of medium particle size, containing pentane as blowing agent. Extir does not contain CFC or HCFC. Extir A 3.. |
|||
Particle Size | 600 - 1000 µm | 600 - 1000 µm | |
Polimeri Europa Extir Leonardo B 3000 AE Expandable Polystyrene
(discontinued **) Extir B 3000 AE is a flame retardant expandable polystyrene in the form of spherical beads of medium particle size, containing pentane as blowing agent. Extir does not contain CFC or HCFC. This grad.. |
|||
Particle Size | 600 - 1000 µm | 600 - 1000 µm | |
Polimeri Europa Extir® D 3000 AE Expandable Polystyrene
(discontinued **) Extir D 3000 AE is a flame-retardant expandable polystyrene in the form of spherical beads of medium particle size, containing pentane as blowing agent. Extir does not contain CFC or CFC. Extir D 30.. |
|||
Particle Size | 600 - 1000 µm | 600 - 1000 µm | |
Polimeri Europa Extir® E 3000 AE Expandable Polystyrene
(discontinued **) Extir E 3000 AE is a flame-retardant expandable polystyrene in the form of spherical beads of medium particle size, with a low pentane content as blowing agent. Extir does not contain CFC or HCFC. T.. |
|||
Particle Size | 600 µm | 600 µm | average; ASTM D4895 |
3M Dyneon™ TF 2072 PTFE
(discontinued **) Processable by standard paste extrusion methodTF 2071 and TF 2072 have a wide processing range because of high maximum allowable reduction ratioTF 2072 is recommended for thin-wall, small diameter t.. |
|||
Particle Size | 600 µm | 600 µm | Weight Average; Sieve Test |
Lucite International Diakon® LG156 Acrylic Bead Polymer, High Transparency PMMA beads offer an exceptional transmission level of 92.5%, an increase of +0.5% in light transmission vs. granular grades - ideal for medical diagnostic devices.Information provided by Lucite Inte.. |
|||
Particle Size | 600 µm | 600 µm | Weight Average; Sieve Test |
Lucite International Diakon® LG702 Acrylic Bead Polymer, High Transparency PMMA beads offer an exceptional transmission level of 92.5%, an increase of +0.5% in light transmission vs. granular grades - ideal for medical diagnostic devices.Information provided by Lucite Inte.. |
|||
Particle Size | 600 µm | 600 µm | Weight Average; Sieve Test |
Lucite International Diakon® LG703 Acrylic Bead Polymer, High Transparency PMMA beads offer an exceptional transmission level of 92.5%, an increase of +0.5% in light transmission vs. granular grades - ideal for medical diagnostic devices.Information provided by Lucite Inte.. |
|||
Particle Size | 600 µm | 600 µm | Weight Average; Sieve Test |
Lucite International Diakon® MH254 Acrylic Bead Polymer, High Transparency PMMA beads offer an exceptional transmission level of 92.5%, an increase of +0.5% in light transmission vs. granular grades - ideal for medical diagnostic devices.Information provided by Lucite Inte.. |
|||
Particle Size | 600 µm | 600 µm | 5 Max % |
Sinotek Materials W75-X Amorphous Graphite Grain Information provided by Sinotek |
|||
Particle Size | 600 µm | 600 µm | Median |
Eliokem Chemigum® P83 Nitrile Elastomer Balanced modifier of plasticized PVC for improved properties and melt processing in the Eliokem product line. 33% bound ACN. Crosslinked polymer structure. PVC partitioning agent.Can be used in P.. |
|||
Particle Size | 600 µm | 600 µm | Median |
Eliokem Chemigum® P8BA Nitrile Elastomer High melt strength. Particularly recommended for extrusion and calendaring. 33% bound ACN. Branched crosslinked polymer structure. PVC partitioning agent.Can be used in PVC blends.Used in automo.. |
|||
Particle Size | 600 µm | 600 µm | Median |
Eliokem Chemigum® P8D Nitrile Elastomer High viscosity grade for friction materials. 33% bound ACN. Branched crosslinked polymer structure. CaCO3 partitioning agent.Can be used in phenolic blends.Used in friction materials such as disc.. |
|||
Particle Size | 600 µm | 600 µm | Median |
Eliokem Chemigum® P35 Nitrile Elastomer Low compression-set for dynamic applications. 35% bound ACN. Crosslinked polymer structure. CaCO3 partitioning agent.Can be used in PVC blends.Used in auto weatherstrips and oil/gas resistant par.. |
|||
Particle Size | 600 µm | 600 µm | Median |
Eliokem Chemigum® P89 Nitrile Elastomer Food contact grade (under specific conditions). 33% bound ACN. Crosslinked polymer structure. PVC partitioning agent.Can be used in PVC blends.Used in food packaging.Information provided by Eliok.. |
|||
Particle Size | 600 µm | 600 µm | <1% above |
BorsodChem ONGRO CPE 3602 C Chlorinated Polyethylene IMPACT MODIFIER FOR PVChigh impact resistancegood processabilityexcellent weather resistanceELASTOMERSvariety of cross-linking technologiesexcellent ozone- and weather resistanceexcellent chemical r.. |
|||
Particle Size | 600 µm | 600 µm | <1% above |
BorsodChem ONGRO CPE 3602 N Chlorinated Polyethylene IMPACT MODIFIER FOR PVChigh impact resistancegood processabilityexcellent weather resistanceELASTOMERSvariety of cross-linking technologiesexcellent ozone- and weather resistanceexcellent chemical r.. |
|||
Particle Size | 600 µm | 600 µm | <1% above |
BorsodChem ONGRO CPE 4002 N Chlorinated Polyethylene IMPACT MODIFIER FOR PVChigh impact resistancegood processabilityexcellent weather resistanceELASTOMERSvariety of cross-linking technologiesexcellent ozone- and weather resistanceexcellent chemical r.. |
|||
Particle Size | 600 µm | 600 µm | Average |
Azoty Tarnow™ TARFLEN SG-2 PTFE Free-Flowing suspension powder for automated compression molding of complicated shapes and isostatic pressing.Information provided by Zakłady Azotowe w Tarnowie-Moscicach S.A. |
|||
Particle Size | 600 µm | 600 µm | Weight Average; Sieve Test |
Lucite International Diakon® MG102 Acrylic Bead Polymer, High Transparency PMMA beads offer an exceptional transmission level of 92.5%, an increase of +0.5% in light transmission vs. granular grades - ideal for medical diagnostic devices.Information provided by Lucite Inte.. |