Polymer Property : Particle Size = 5500 µm Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Particle Size <= 5500 µm
<= 5500 µm
BASF Neopolen® P 8225 K 0.025 g/cc Core density; Expanded Polypropylene (Europe)
Description: Neopolen® P 8225 K is expanded Polypropylene supplied in the form of beads. The cells are largely closed.Physical properties of moldings made from Neopolen® P 8225 K.Note: In order to..
Particle Size <= 5500 µm
<= 5500 µm
BASF Neopolen® P 8225 K 0.03 g/cc Core density; Expanded Polypropylene (Europe)
Description: Neopolen® P 8225 K is expanded Polypropylene supplied in the form of beads. The cells are largely closed.Physical properties of moldings made from Neopolen® P 8225 K.Note: In order to..
Particle Size <= 5500 µm
<= 5500 µm
BASF Neopolen® P 8225 K 0.04 g/cc Core density; Expanded Polypropylene (Europe)
Description: Neopolen® P 8225 K is expanded Polypropylene supplied in the form of beads. The cells are largely closed.Physical properties of moldings made from Neopolen® P 8225 K.Note: In order to..
Particle Size <= 5500 µm
<= 5500 µm
BASF Neopolen® P 8225 K 0.05 g/cc Core density; Expanded Polypropylene (Europe)
Description: Neopolen® P 8225 K is expanded Polypropylene supplied in the form of beads. The cells are largely closed.Physical properties of moldings made from Neopolen® P 8225 K.Note: In order to..