Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Particle Size = 55 µm Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Particle Size 35 - 55 µm
35 - 55 µm
Lucite International Colacryl ® TS1742 Acrylic Dental Resin
Lucite® Colacryl® TS1742 is a plasticiser free, ethyl methacrylate based resin aimed at the formulation of heat-cured, soft materials, such as ear moulds, where it is well suited to use with C..
Particle Size 45 - 55 µm
45 - 55 µm
Lucite International Colacryl ® TS1785 Acrylic Dental Resin
Cold-curing denture repair resin with Methyl Methacrylate based copolymers. Features fast polymerisation, easy mixing, good clarity, short hydroflask cure cycles, and excellent pigment acceptance.I..
Particle Size 40 - 55 µm
40 - 55 µm
d90, Guaranteed
TIMCAL TIMREX® LSG 44 Natural Graphite Flakes
TIMREX Natural Flake Graphite is produced in a wide range of products distinguished by particle size distribution, chemistry and carbon content. Timcal mines the graphite from its own source in Lac-..
Particle Size 35 - 55 µm
35 - 55 µm
D(0.5)
Akzo Nobel Expancel® 091 WE 40 d24 Wet expanded microspheres
Expancel microspheres are thermoplastic hollow spheres. The microspheres are white spherically formed particles with a thermoplastic shell encapsulating a gas. When the microspheres are heated the..
Particle Size 35 - 55 µm
35 - 55 µm
D(0.5)
Akzo Nobel Expancel® 461 DE 40 d25 Dry expanded microspheres
Expancel microspheres are thermoplastic hollow spheres. The microspheres are white spherically formed particles with a thermoplastic shell encapsulating a gas. When the microspheres are heated the..
Particle Size 35 - 55 µm
35 - 55 µm
D(0.5)
Akzo Nobel Expancel® 461 DET 40 d25 Dry expanded microspheres
Expancel microspheres are thermoplastic hollow spheres. The microspheres are white spherically formed particles with a thermoplastic shell encapsulating a gas. When the microspheres are heated the..
Particle Size 35 - 55 µm
35 - 55 µm
D(0.5)
Akzo Nobel Expancel® 091 DE 40 d30 Dry expanded microspheres
Expancel microspheres are thermoplastic hollow spheres. The microspheres are white spherically formed particles with a thermoplastic shell encapsulating a gas. When the microspheres are heated the..
Copyright © lookpolymers.com All Rights Reserved