Polymer Property : Particle Size = 50.0 µm Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Particle Size 20.0 - 50.0 µm
20.0 - 50.0 µm
Average value: 32.0 µm Grade Count:5
Overview of materials for Epoxy Adhesive
This property data is a summary of similar materials in the MatWeb database for the category "Epoxy Adhesive". Each property range of values reported is minimum and maximum values of appropriate Mat..
Particle Size 2.00 - 50.0 µm
2.00 - 50.0 µm
Average value: 30.4 µm Grade Count:43
Overview of materials for Epoxy, Electrically Conductive
This property data is a summary of similar materials in the MatWeb database for the category "Epoxy, Electrically Conductive". Each property range of values reported is minimum and maximum values of..
Particle Size 5.00 - 50.0 µm
5.00 - 50.0 µm
Average value: 27.5 µm Grade Count:3
Overview of materials for Low Density Polyethylene (LDPE), Molded
This property data is a summary of similar materials in the MatWeb database for the category "Low Density Polyethylene (LDPE), Molded". Each property range of values reported is minimum and maximum ..