Polymer Property : Particle Size = 340 µm
Polymer Property :
Particle Size =
340 µm
Product List
Physical Properties
Tips:
30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties
Metric
English
Comments
Particle Size
240
-
340
µm
240
-
340
µm
Dow Method
Dow Saran® 168
Information provided by Dow