Polymer Property : Particle Size = 280 µm Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Particle Size 280 µm
280 µm
Dow Method
Dow XU 32019.10 Barrier Polymer
Excellent oxygen and water vapor barrier Information provided by Dow
Particle Size 280 µm
280 µm
Dow Method
Dow XU 32046.31 Barrier Polymer
Excellent oxygen and water vapor barrier Information provided by Dow