Polymer Property : Particle Size = 2.50 µm Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Particle Size 1.50 - 2.50 µm
1.50 - 2.50 µm
Average value: 1.83 µm Grade Count:3
Overview of materials for Linear Low Density Polyethylene (LLDPE), Blow Molding Grade
This property data is a summary of similar materials in the MatWeb database for the category "Linear Low Density Polyethylene (LLDPE), Blow Molding Grade". Each property range of values reported is ..
Particle Size 1.50 - 2.50 µm
1.50 - 2.50 µm
Average value: 1.83 µm Grade Count:3
Overview of materials for Linear Low Density Polyethylene (LLDPE), Sheeting Grade
This property data is a summary of similar materials in the MatWeb database for the category "Linear Low Density Polyethylene (LLDPE), Sheeting Grade". Each property range of values reported is mini..