Physical Properties Metric English Comments
Particle Size 700 - 1000 µm
700 - 1000 µm
Polimeri Europa Extir® LN 3000 Expandable Polystyrene
Extir LN 3000 belongs to a new expandable product family, the Leonardo Series, with improved processing features: high expandability, high moulding productivity, wide processing area, optimal fusion..
Particle Size 600 - 1000 µm
600 - 1000 µm
Polimeri Europa Extir® Verdi VR A3000 AE Expandable Polystyrene - Flame Retardant
Product Description:Extir Verdi VR A3000 AE is a flame-retardant expandable polystyrene in the form of spherical beads of medium particle size, containing pentane as blowing agent.Extir does not con..
Particle Size 600 - 1000 µm
600 - 1000 µm
Polimeri Europa Extir® D 3000 AE Expandable Polystyrene - Flame Retardant
Product Description:Extir D 3000 AE is a flame-retardant expandable polystyrene in the form of spherical beads of medium particle size, containing pentane as blowing agent.Extir does not contain CFC..
Particle Size 600 - 1000 µm
600 - 1000 µm
Polimeri Europa Extir® GEO 3000 AE Expandable Polystyrene - Flame Retardant
Product Description:Extir GEO 3000 AE is a flame-retardant expandable polystyrene in the form of spherical beads of medium particle size, containing pentane as blowing agent.Extir does not contain C..
Particle Size 600 - 1000 µm
600 - 1000 µm
Polimeri Europa Extir Leonardo A 3000 AE Expandable Polystyrene  (discontinued **)
Extir A 3000 AE is a flame retardant expandable polystyrene in the form of spherical beads of medium particle size, containing pentane as blowing agent. Extir does not contain CFC or HCFC. Extir A 3..
Particle Size 600 - 1000 µm
600 - 1000 µm
Polimeri Europa Extir Leonardo B 3000 AE Expandable Polystyrene  (discontinued **)
Extir B 3000 AE is a flame retardant expandable polystyrene in the form of spherical beads of medium particle size, containing pentane as blowing agent. Extir does not contain CFC or HCFC. This grad..
Particle Size 600 - 1000 µm
600 - 1000 µm
Polimeri Europa Extir® D 3000 AE Expandable Polystyrene  (discontinued **)
Extir D 3000 AE is a flame-retardant expandable polystyrene in the form of spherical beads of medium particle size, containing pentane as blowing agent. Extir does not contain CFC or CFC. Extir D 30..
Particle Size 600 - 1000 µm
600 - 1000 µm
Polimeri Europa Extir® E 3000 AE Expandable Polystyrene  (discontinued **)
Extir E 3000 AE is a flame-retardant expandable polystyrene in the form of spherical beads of medium particle size, with a low pentane content as blowing agent. Extir does not contain CFC or HCFC. T..
Particle Size 5.00 - 1000 µm
5.00 - 1000 µm
Average value: 494 µm Grade Count:7
Overview of materials for Ethylene Vinyl Acetate Copolymer (EVA), Molded/Extruded
This property data is a summary of similar materials in the MatWeb database for the category "Ethylene Vinyl Acetate; Molded/Extruded". Each property range of values reported is minimum and maximum ..
Particle Size 500 - 1000 µm
500 - 1000 µm
50% Min; 540MA3C5E
Solvay MIRAPOL® SURF-S 410 Surfactant
Description: Granulated rinse aid polymer for use in automatic dish washing powders or tablets. 18% activeIdentification: BLEND OF ACRYLIC BASED POLYMER AND SODIUM TRIPOLYPHOSPHATE.Use level : 0.5 â..
Particle Size 710 - 1000 µm
710 - 1000 µm
min 92%; BC HSZ 326:2001/1 screening
BorsodChem ONGROSTYR F-II Expandable Polystyrene (EPS)
ONGROSTYR F-II is an expandable, flame-retardant styrene homopolymer, produced by suspension polymerization. The product meets the requirements of DIN 4102 and of B1 class of building materials, i.e..