Physical Properties | Metric | English | Comments |
---|---|---|---|
Particle Size | 700 - 1000 µm | 700 - 1000 µm | |
Polimeri Europa Extir® LN 3000 Expandable Polystyrene Extir LN 3000 belongs to a new expandable product family, the Leonardo Series, with improved processing features: high expandability, high moulding productivity, wide processing area, optimal fusion.. |
|||
Particle Size | 600 - 1000 µm | 600 - 1000 µm | |
Polimeri Europa Extir® Verdi VR A3000 AE Expandable Polystyrene - Flame Retardant Product Description:Extir Verdi VR A3000 AE is a flame-retardant expandable polystyrene in the form of spherical beads of medium particle size, containing pentane as blowing agent.Extir does not con.. |
|||
Particle Size | 600 - 1000 µm | 600 - 1000 µm | |
Polimeri Europa Extir® D 3000 AE Expandable Polystyrene - Flame Retardant Product Description:Extir D 3000 AE is a flame-retardant expandable polystyrene in the form of spherical beads of medium particle size, containing pentane as blowing agent.Extir does not contain CFC.. |
|||
Particle Size | 600 - 1000 µm | 600 - 1000 µm | |
Polimeri Europa Extir® GEO 3000 AE Expandable Polystyrene - Flame Retardant Product Description:Extir GEO 3000 AE is a flame-retardant expandable polystyrene in the form of spherical beads of medium particle size, containing pentane as blowing agent.Extir does not contain C.. |
|||
Particle Size | 600 - 1000 µm | 600 - 1000 µm | |
Polimeri Europa Extir Leonardo A 3000 AE Expandable Polystyrene
(discontinued **) Extir A 3000 AE is a flame retardant expandable polystyrene in the form of spherical beads of medium particle size, containing pentane as blowing agent. Extir does not contain CFC or HCFC. Extir A 3.. |
|||
Particle Size | 600 - 1000 µm | 600 - 1000 µm | |
Polimeri Europa Extir Leonardo B 3000 AE Expandable Polystyrene
(discontinued **) Extir B 3000 AE is a flame retardant expandable polystyrene in the form of spherical beads of medium particle size, containing pentane as blowing agent. Extir does not contain CFC or HCFC. This grad.. |
|||
Particle Size | 600 - 1000 µm | 600 - 1000 µm | |
Polimeri Europa Extir® D 3000 AE Expandable Polystyrene
(discontinued **) Extir D 3000 AE is a flame-retardant expandable polystyrene in the form of spherical beads of medium particle size, containing pentane as blowing agent. Extir does not contain CFC or CFC. Extir D 30.. |
|||
Particle Size | 600 - 1000 µm | 600 - 1000 µm | |
Polimeri Europa Extir® E 3000 AE Expandable Polystyrene
(discontinued **) Extir E 3000 AE is a flame-retardant expandable polystyrene in the form of spherical beads of medium particle size, with a low pentane content as blowing agent. Extir does not contain CFC or HCFC. T.. |
|||
Particle Size | 5.00 - 1000 µm | 5.00 - 1000 µm | Average value: 494 µm Grade Count:7 |
Overview of materials for Ethylene Vinyl Acetate Copolymer (EVA), Molded/Extruded This property data is a summary of similar materials in the MatWeb database for the category "Ethylene Vinyl Acetate; Molded/Extruded". Each property range of values reported is minimum and maximum .. |
|||
Particle Size | 500 - 1000 µm | 500 - 1000 µm | 50% Min; 540MA3C5E |
Solvay MIRAPOL® SURF-S 410 Surfactant Description: Granulated rinse aid polymer for use in automatic dish washing powders or tablets. 18% activeIdentification: BLEND OF ACRYLIC BASED POLYMER AND SODIUM TRIPOLYPHOSPHATE.Use level : 0.5 â.. |
|||
Particle Size | 710 - 1000 µm | 710 - 1000 µm | min 92%; BC HSZ 326:2001/1 screening |
BorsodChem ONGROSTYR F-II Expandable Polystyrene (EPS) ONGROSTYR F-II is an expandable, flame-retardant styrene homopolymer, produced by suspension polymerization. The product meets the requirements of DIN 4102 and of B1 class of building materials, i.e.. |