Physical Properties | Metric | English | Comments |
---|---|---|---|
Particle Size | 1.53 µm | 1.53 µm | |
Dow Latex LXC 771NA Carboxylated Styrene-Butadiene Latex Applications: Dow Latex LXC 771NA is a high solids, high performance latex that offers many benefits over standard styrene-butadiene latexes in carpet applications. Dow Latex LXC 771NA is a unique p.. |