Particle Size 0.90 µm
0.90 µm
Median
Nabaltec ACTILOX® B60 AS1 AlO(OH) Boehmite
Surface treated flame retardant filler with reduced particle size and optimized viscosity in engineering plastics for synergistic effects with other flame retardants.Properties:Very fine product in ..
Particle Size 0.90 µm
0.90 µm
Median Grain Diameter
Nabaltec APYRAL® 120E Al(OH)3
APYRAL ® from Nabaltec is an environmentally friendly halogen free product which is used as a flame retardant filler in a wide variety of rubber and polymeric materials. During thermal decompositio..
Particle Size 0.90 µm
0.90 µm
Median; Laser Diffraction
Nabaltec APYRAL® AOH 60 AlO(OH) Boehmite
Mineral flame retardant for wire and cable industry, electronic industry and public transport.Properties:High temperature applicationsLow sedimentation at good viscosity performance in resinsGood ch..
Particle Size <= 0.90 µm
<= 0.90 µm
Average Particle Size/Laser Diffraction D50
H.C. Starck Grade C Yttrium Oxide
Sintering additive for Si3N4 and ALNStabilizer for zirconias (PSZ) and insulating coatings (TBC`s)Catalyst carrierYttria stabilized zirconias electrolytes for solid oxide fuel cellsLuminescent mater..
Particle Size 0.90 µm
0.90 µm
Rubber Particle Size
UBE C (Low-Cis) HIPS (n-DM = 0.03 wt % and PH-3H = 0.03 wt %)
Description: UBE high impact polystyrene (HIPS).Information provided by UBE.
Particle Size 0.90 - 1.3 µm
0.90 - 1.3 µm
D50 (Malvern)
Vesta Ceramics SicoNide® P Silicon Nitride Powder
General Description:SicoNide® is a silicon nitride powder with a broad particle size distribution allowing better, tighter packing when pressed. Our computer-controlled production processes guaran..
Particle Size 0.90 - 1.3 µm
0.90 - 1.3 µm
D50 (Malvern)
Vesta Ceramics SicoNide® S S Silicon Nitride Powder
General Description:SicoNide® is a silicon nitride powder with a broad particle size distribution allowing better, tighter packing when pressed. Our computer-controlled production processes guaran..
Particle Size 0.90 µm
0.90 µm
Median; Laser Diffraction
Nabaltec ACTILOX® B60 AlO(OH) Boehmite
Mineral flame retardant for wire and cable industry, electronic industry and public transport.Properties:High temperature stabilitySynergistic effects with other flame retardantsHigh acid resistance..
Particle Size 0.90 µm
0.90 µm
Rubber Particle Size
UBE A (High-Cis) HIPS (n-DM = 0.03 wt % and PH-3H = 0.03 wt %)
Description: UBE high impact polystyrene (HIPS).Information provided by UBE.
Particle Size 0.90 µm
0.90 µm
Rubber Particle Size
UBE UBEPOL BR15HB HIPS (n-DM = 0.03 wt % and PH-3H = 0.03 wt %)
Description: UBEPOL-BR15HB is characterized by the highest branching of these 3 grades and is adapted by many PS manufacturers.Information provided by UBE.