Polymer Property : Particle Size = 0.37 µm Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Particle Size 0.37 µm
0.37 µm
Median particle diameter
Old Hickory M-23 Tennessee Ball Clay
This is a very high quality porcelain grade ball clay. It has fine particle size distribution for excellent plasticity and strength in pressing or plastic forming application. the low Fe2O3 and TiO2..
Particle Size 0.37 µm
0.37 µm
Median particle diameter
Old Hickory No. 1 Glaze Kentucky Ball Clay
No. 1 Glaze Clay is a very high kaolin bearing selection with extremely low levels of carbon content. it provides excellent suspension to all types of glazes especially glazes containing a high perc..