Physical Properties | Metric | English | Comments |
---|---|---|---|
Particle Size | 0.16 µm | 0.16 µm | average; DIN ISO 13321 |
3M Dyneon™ TF 5032R PTFE
(discontinued **) Small particle sizeExcellent penetrating propertiesLow settling tendencyInformation provided by Dyneon, A 3M Company |
|||
Particle Size | 0.16 µm | 0.16 µm | |
Mallard Creek Polymers ROVENE® 4041 SBR Latex ROVENE® 4041 is a freeze-thaw stable carboxylated styrene-butadiene emulsion that can be used as a modifier for concrete applications. Concrete modified with ROVENE® 4041 is much tougher, more.. |
|||
Particle Size | 0.16 µm | 0.16 µm | |
Mallard Creek Polymers ROVENE® 4151 SBR Latex ROVENE® 4151 is a carboxylated styrene-butadiene emulsion that has a soft, resilient hand with above average strength properties. It may be compounded with a wide variety of fillers and additives.. |
|||
Particle Size | 0.16 µm | 0.16 µm | |
Mallard Creek Polymers ROVENE® 4306 SBR Latex ROVENE® 4306 is a carboxylated styrene-butadiene emulsion that has a soft, resilient hand with outstanding strength properties. This self-crosslinking binder imparts excellent water and solvent r.. |
|||
Particle Size | 0.16 µm | 0.16 µm | |
Mallard Creek Polymers ROVENE® 4813 SBR Emulsion ROVENE® 4813 is a high gel content hot polymerized SBR latex with 30% bound styrene content. It has excellent shear stability and high tolerance for fillers and pH shock. It is easily tackified a.. |
|||
Particle Size | 0.16 µm | 0.16 µm | |
Mallard Creek Polymers ROVENE® 5044 SBR Latex ROVENE® 5044 is a very soft carboxylated styrene - butadiene (SBR) latex emulsion specifically designed for formulation of permanent label and construction adhesives. Its relative low molecular w.. |
|||
Particle Size | 0.16 µm | 0.16 µm | |
Mallard Creek Polymers Rovene® 5499 Styrene-Butadiene Emulsion Rovene® 5499 is a styrene-butadiene emulsion that was developed as an ink vehicle for TPO based wall coverings. More specifically it can be formulated for metallic ink vehicles. Rovene® 5499 p.. |
|||
Particle Size | 0.16 µm | 0.16 µm | |
Mallard Creek Polymers ROVENE® 6066 Styrene-Acrylic Latex Applications: Rovene® 6066 is specifically designed for formulation of binder systems for moldable and self supporting composites. Its molecular weight allows formulation latitude for many ‘.. |
|||
Particle Size | 0.16 µm | 0.16 µm | |
Mallard Creek Polymers ROVENE® 9410 SBR Latex ROVENE® 9410 is a very soft carboxylated styrene - butadiene (SBR) latex emulsion. Its relative high molecular weight and styrene content (25%) permits the formulation of pressure sensitive adhes.. |
|||
Particle Size | 0.16 µm | 0.16 µm | |
Mallard Creek Polymers ROVENE® 4423 SBR Latex ROVENE® 4423 is a very soft carboxylated styrene - butadiene (SBR) latex emulsion specifically designed for formulation of permanent label adhesives. Its relative high molecular weight and styren.. |