Physical Properties | Metric | English | Comments |
---|---|---|---|
Bulk Density | 2.93 g/cc | 0.106 lb/in³ | |
Poco Graphite SUPERSiC® Si Silicon Carbide The SUPERSiC Material System allows customization of basic silicon carbide. Select from groups of infiltration materials, cleaning options, coating materials and thicknesses to optimize material for.. |
|||
Bulk Density | 2.93 g/cc | 0.106 lb/in³ | |
Chosun Refractories A18H Magnesia Carbon Bricks for Electric Arc Furnace Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Bulk Density | 2.93 g/cc | 0.106 lb/in³ | |
Chosun Refractories A18HM Magnesia Carbon Bricks for Electric Arc Furnace Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Bulk Density | 2.93 g/cc | 0.106 lb/in³ | |
Chosun Refractories A18S Magnesia Carbon Bricks for Electric Arc Furnace Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |