Physical Properties | Metric | English | Comments |
---|---|---|---|
Bulk Density | 2.50 g/cc | 0.0903 lb/in³ | |
MarkeTech Repton 504 Mullite Brand 504 features: Max spall resistance.REPTON setter tiles, kiln furniture, and special fixtures are lightweight, ridge, and high strength ceramics that resist distortion and spalling, even when t.. |
|||
Bulk Density | 2.50 g/cc | 0.0903 lb/in³ | |
McDanel Advanced Ceramics MV-20 Mullite Information provided by McDanel Advanced Ceramic Technologies |
|||
Bulk Density | 2.50 - 2.60 g/cc | 0.0903 - 0.0939 lb/in³ | After drying at 110°C |
Gouda Vuurvast CURAS SiC 90 D Moldable Refractory Material Description: This material is supplied as a dry powder. It has to be mixed with clean water to the necessary consistency. Curas SiC 90 has a phosphate bond and especially meant for protection of bo.. |
|||
Bulk Density | 2.50 - 2.60 g/cc | 0.0903 - 0.0939 lb/in³ | After drying at 110°C |
Gouda Vuurvast CURON 160 C Dense Refractory Castable Description: Because of the selection of raw materials this castable has a high volume stability and keeps its strength up to high temperatures. In addition Curon 160 C has an excellent thermal shoc.. |
|||
Bulk Density | 2.50 - 2.60 g/cc | 0.0903 - 0.0939 lb/in³ | After drying at 110°C |
Gouda Vuurvast CURON 120 S Dense Refractory Castable Description: A very strong castable with a high abrasion resistance of which both aggregate and cement attribute to hydraulic binding.Remarks: These values apply to cast products. Also available in .. |
|||
Bulk Density | 2.50 - 2.60 g/cc | 0.0903 - 0.0939 lb/in³ | After drying at 110°C |
Gouda Vuurvast CURON 13 S Dense Refractory Castable Description: Curon 13 S is a spinel based castable with a very low silica content and therefore it is suitable for direct contact with all kinds of aluminum/alloys and fluxes in aluminum melting/hol.. |
|||
Bulk Density | 2.50 - 2.60 g/cc | 0.0903 - 0.0939 lb/in³ | After drying at 110°C |
Gouda Vuurvast CURON 13 SC Dense Refractory Castable Description: Curon 13 SC is a spinel based castable with a very low silica content and therefore it is suitable for direct contact with all kinds of aluminum/alloys and fluxes in aluminum melting/ho.. |
|||
Bulk Density | 2.50 - 2.60 g/cc | 0.0903 - 0.0939 lb/in³ | After drying at 110°C |
Gouda Vuurvast CURON 14 S Dense Refractory Castable Description: Curon 14 S is a dense, strong and abrasion resistant castable. Because of the very low percentage of Fe2O3 and SiO2 it is used for highly abrasive conditions in reducing atmospheres.Rem.. |
|||
Bulk Density | 2.50 - 2.60 g/cc | 0.0903 - 0.0939 lb/in³ | After drying at 110°C |
Gouda Vuurvast CURON 150 Dense Refractory Castable Description: This bauxite based castable has a very good thermal shock resistance and is therefore well suited for burner blocks.Remarks: These values apply to cast products. Also available in gunni.. |
|||
Bulk Density | 2.50 - 2.60 g/cc | 0.0903 - 0.0939 lb/in³ | After drying at 110°C |
Gouda Vuurvast VIBRON 160 H RAPID Dense Vibrating Refractory Castable Description: Vibron 160 H Rap is a low cement castable based on high fired high alumina grog and characterized by a high strength and good thermal shock resistance. Because of special additives, thi.. |
|||
Bulk Density | 2.50 g/cc | 0.0903 lb/in³ | |
Sharadaa Ceramics HA 60 High Alumina Brick Services Offered: Retrofitting of Furnace, Installation of Castables/Bricks/Ceramic Fiber Modules, Castable Laying by Vibrocasting/Guiniting, Turnkey Installation Boiler/Chimney/Heater/Reformer/Rota.. |
|||
Bulk Density | 2.50 g/cc | 0.0903 lb/in³ | |
Sharadaa Ceramics HA 62D High Alumina Brick Services Offered: Retrofitting of Furnace, Installation of Castables/Bricks/Ceramic Fiber Modules, Castable Laying by Vibrocasting/Guiniting, Turnkey Installation Boiler/Chimney/Heater/Reformer/Rota.. |
|||
Bulk Density | 2.50 g/cc | 0.0903 lb/in³ | After Drying at 110°C |
Sharadaa Ceramics PCF (SIC) Precast Prefired Brick Features: Manufactured under controlled conditions under refractory engineers supervision; Measured Quantity/Temperature of water, mixing by Intensive counter current mixers, Forming by Vibro Castin.. |
|||
Bulk Density | >= 2.50 g/cc | >= 0.0903 lb/in³ | Sample, cast, cured, dried at 110°C |
Sharadaa Ceramics REFCAST SUPER Dense Castables Description: We offer a range of Dense Castables that are conventional castable and extensively used in boiler work, general furnace and burner blocks. Made as per international standards, our range.. |
|||
Bulk Density | >= 2.50 g/cc | >= 0.0903 lb/in³ | Sample, cast, cured, dried at 110°C |
Sharadaa Ceramics THERMO PATCH Dense Castables Description: We offer a range of Dense Castables that are conventional castable and extensively used in boiler work, general furnace and burner blocks. Made as per international standards, our range.. |
|||
Bulk Density | 2.50 g/cc | 0.0903 lb/in³ | After Drying at 110°C |
Sharadaa Ceramics VELECRETE RC 103 Rodding Castables Description: The Rodding Castables offered by us are user friendly in nature and does not require high energy mixing machines and vibrators. Free flowing in nature, these castables are designed in c.. |
|||
Bulk Density | 2.50 g/cc | 0.0903 lb/in³ | |
Sharadaa Ceramics MULL Mullite Services Offered: Retrofitting of Furnace, Installation of Castables/Bricks/Ceramic Fiber Modules, Castable Laying by Vibrocasting/Guiniting, Turnkey Installation Boiler/Chimney/Heater/Reformer/Rota.. |
|||
Bulk Density | 2.50 - 2.60 g/cc | 0.0903 - 0.0939 lb/in³ | |
Chosun Refractories CUN-669 Nozzle Brick Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Bulk Density | 2.50 g/cc | 0.0903 lb/in³ | |
Chosun Refractories HSC-16HW Casting Block Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Bulk Density | 2.50 g/cc | 0.0903 lb/in³ | |
Chosun Refractories SAL60 Special Alumina brick Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Bulk Density | 2.50 g/cc | 0.0903 lb/in³ | |
Chosun Refractories SBSN-G15 Nozzle Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Bulk Density | 2.50 g/cc | 0.0903 lb/in³ | Scott |
China Tungsten YG15X Tungsten Carbide Powder Information provided by China Tungsten |
|||
Bulk Density | >= 2.50 g/cc | >= 0.0903 lb/in³ | |
China-Yixing Longly Refractories Seggar Semi-Corundum-Mullite Our company's production of a variety of corundum mullite push slab (moved plate), corundum-mullite seggar, corundum mullite corrugated board and other kinds of the kiln furniture, high refractorine.. |
|||
Bulk Density | 2.50 - 2.60 g/cc | 0.0903 - 0.0939 lb/in³ | After drying at 110°C |
Gouda Vuurvast FLUCON 160 H Dense Self Flowing Refractory Castable Description: Flucon 160 H is a self-flowing low cement castable on high fired high alumina grog base, characterized by a high strength and good thermal shock resistance.Remarks: These values apply t.. |