Polymer Property : Bulk Density = 1.43 g/cc Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Bulk Density 1.43 - 1.59 g/cc
0.0517 - 0.0574 lb/in³
3M #11 Filtration Granule (Corona)
3M #11 Filtration Granules are natural minerals used for water filtration in irrigation system.Information provided by 3M
Bulk Density 1.43 - 1.59 g/cc
0.0517 - 0.0574 lb/in³
3M Headlap Roofing Granule (Corona)
3M Headlap Roofing Granules are ceramic-coated or natural minerals used as headlap surfacing material in asphalt roofing products. These granules are treated to promote adhesion to asphalt. These He..