Physical Properties | Metric | English | Comments |
---|---|---|---|
Bulk Density | 1.12 g/cc | 0.0405 lb/in³ | Tapped |
Nyco NYAD G® WOLLASTOCOAT® Wollastonite Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctive particle morphology makes wollastonite an ideal performance mineral for a br.. |
|||
Bulk Density | 1.12 g/cc | 0.0405 lb/in³ | packed |
Imerys Minsparâ„¢ 200 Feldspar Minspar 200 is 200 mesh flotation grade soda Feldspar used in the ceramic whiteware industry for sanitaryware, dinnerware, floor and wall tile, artware and glazes.Information provided by Imerys |
|||
Bulk Density | 1.12 g/cc | 0.0405 lb/in³ | packed |
Imerys Minsparâ„¢ 3 Ground Feldspar Minsparâ„¢ 3 is a coarse particle size, ground Feldspar with a tightly controlled particle size distribution. The angular particle shape and inherent cheMical resistance make Minsparâ„¢ 3 an e.. |
|||
Bulk Density | 1.12 g/cc | 0.0405 lb/in³ | Standard |
GrafTech GRAFIHX® RXS Series Flexible Graphite Heat Transfer Plates GRAFIHX® RXS Series are heat transfer plates for radiant heating applications made from high thermal conductivity flexible graphite. They are available in rolls and sheets as a replacement for tr.. |
|||
Bulk Density | 1.12 g/cc | 0.0405 lb/in³ | Available |
GrafTech GRAFOIL® GHC Standard Internal Combustion Laminate GRAFOIL® Grade GHC is a laminate made from Grade GTC flexible graphite. Laminate Construction: GRAFOIL® Grade GTC ? Micro-thin, phenolic-based adhesive ? GRAFOIL® Grade GTC |
|||
Bulk Density | 1.12 g/cc | 0.0405 lb/in³ | Standard; Graphite |
GrafTech GRAFOIL® GHE Standard Fluid Sealing Laminate, Metal Reinforced GRAFOIL® Grade GHE laminate is made with GTB flexible graphite mechanically bonded to both faces of a 316 or 316L stainless steel tang metal insert. Surface identifiable, the laminate is branded .. |
|||
Bulk Density | 1.12 g/cc | 0.0405 lb/in³ | Standard; Graphite |
GrafTech GRAFOIL® GHH Standard Internal Combustion Laminate, Metal Reinforced GRAFOIL® Grade GHH is a laminate made with GRAFOIL® Grade GTC flexible graphite chemically bonded to both faces of a flat, low-carbon steel core. Its applications include: exhaust sealing, ga.. |
|||
Bulk Density | 1.12 g/cc | 0.0405 lb/in³ | Standard; Graphite |
GrafTech GRAFOIL® GHJ Non-Standard Internal Combustion Grade GHJ Laminate, Metal Reinforced GRAFOIL® Grade GHJ is a laminate made with GRAFOIL® Grade GTC flexible graphite mechanically attached to a perforated, low-carbon steel core. Its applications include: exhaust manifold gasket.. |
|||
Bulk Density | 1.12 g/cc | 0.0405 lb/in³ | Standard; Graphite |
GrafTech GRAFOIL® GHL Standard Fluid Sealing Grade GHL Laminate GRAFOIL® Grade GHL is a laminate made with GRAFOIL® Grade GTB flexible graphite. Laminate thicknesses > 0.060" will be adhesively bonded to final thickness. Laminate thicknesses |
|||
Bulk Density | 1.12 g/cc | 0.0405 lb/in³ | Standard; Graphite |
GrafTech GRAFOIL® GHR Standard Fluid Sealing Laminate, Metal Reinforced GRAFOIL® Grade GHR is an uncured laminate made with GRAFOIL® Grade GTB flexible graphite adhesively bonded to both faces of a 0.002" thick flat 316 or 316L stainless steel insert. Surface iden.. |
|||
Bulk Density | 1.12 g/cc | 0.0405 lb/in³ | Standard; Graphite |
GrafTech GRAFOIL® GHW Standard Fluid Sealing Laminate, Non-Metal Reinforced GRAFOIL® Grade GHW is a laminate made with GRAFOIL® Grade GTB flexible graphite thermally bonded to a 0.0025" thick high-temperature continuous woven glass fiber insert. Its functional tempera.. |
|||
Bulk Density | 1.12 g/cc | 0.0405 lb/in³ | Standard |
GrafTech GRAFOIL® GTA Standard Fluid Sealing Graphite Single Layer Gasketing Material GRAFOIL® GTA premium flexible graphite is a non-inhibited grade developed for use in nuclear or semiconductor applications. It is certified to meet the most rigorous purity specifications of the .. |
|||
Bulk Density | 1.12 g/cc | 0.0405 lb/in³ | Standard for 0.005", 0.010", 0.015", 0.020", 0.025", 0.030", 0.060" thick |
GrafTech GRAFOIL® GTB Standard Fluid Sealing Graphite Single Layer Gasketing Material GRAFOIL® GTB flexible graphite sheet is a gasketing material containing no binders or fillers. Standard industrial grade GTB flexible graphite has an oxidation/corrosion inhibitor and is typicall.. |
|||
Bulk Density | 1.12 g/cc | 0.0405 lb/in³ | Standard |
GrafTech GRAFOIL® GTC Standard Internal Combustion Graphite, Single Layer Material GRAFOIL® GTC flexible graphite sheet is a gasketing material containing no binders or fillers, which will seal a wide variety of liquids and gases over an extremely large temperature range. GTC c.. |
|||
Bulk Density | 1.12 g/cc | 0.0405 lb/in³ | Standard; Graphite |
GrafTech GRAFOIL® GTH Standard Fluid Sealing Adhesive-Backed Tape, Gasket and Thread Tape GRAFOIL® Grade GTH is a pressure sensitive adhesive-backed tape made with GRAFOIL® Grade GTB flexible graphite. It applications include: threaded joints, forming place gaskets, and large diam.. |
|||
Bulk Density | 1.12 g/cc | 0.0405 lb/in³ | Standard |
GrafTech GRAFOIL® GTJ Standard Fluid Sealing Graphite, Single Layer Material GRAFOIL® GTJ premium flexible graphite is an oxidation/corrosion inhibited grade developed for use in nuclear and high temp, high purity applications. It is certified to meet the most rigorous pu.. |
|||
Bulk Density | 1.12 g/cc | 0.0405 lb/in³ | Standard |
GrafTech GRAFOIL® GTX Standard Fluid Sealing Graphite, Single Layer Material GRAFOIL® GTX flexible graphite sheet is inhibited for high oxidation/corrosion resistance that can be used for most fluid sealing and industrial applications. Grade GTX contains an inorganic, non.. |
|||
Bulk Density | 1.12 g/cc | 0.0405 lb/in³ | Standard |
GrafTech GRAFOIL® SUPER GTO® Standard Internal Combustion Single Layer Gasketing Material GRAFOIL® SUPER GTO® flexible graphite sheet is a gasketing material containing no binders, which will seal a wide variety of liquids and gases over an extremely large temperature range (-240Â.. |
|||
Bulk Density | 1.12 g/cc | 0.0405 lb/in³ | Standard; Graphite |
GrafTech GRAFOIL® TG-251 Standard Internal Combustion Laminate, Metal Reinforced GRAFOIL® Grade TG-251 is GRAFOIL® Grade GTC flexible graphite chemically bonded to both faces of a flat, low-carbon steel core. Its applications include: exhaust sealing, gasoline/diesel head.. |
|||
Bulk Density | 1.12 g/cc | 0.0405 lb/in³ | Available |
GrafTech GRAFOIL® TG-411 Non-Standard Fluid Sealing Graphite, High Temperature GRAFOIL® TG-411 is a high temperature purified flexible graphite sheet for applications that require extremely low impurity levels. Material greater than 0.040" (1 mm) thick is adhesively bonded .. |
|||
Bulk Density | 1.12 g/cc | 0.0405 lb/in³ | Standard; Graphite |
GrafTech GRAFOIL® GRAFKOTE® Laminates, Non-Metal Reinforced GRAFOIL® GRAFKOTE® laminates are made with GRAFOIL® Grade GTB flexible graphite thermally bonded to a 0.0005" thick polymer facing on one ("Single-Sided") or both ("Double-Sided") sides. Th.. |
|||
Bulk Density | 1.12 g/cc | 0.0405 lb/in³ | Packed |
Excalibar ExCal® 400 Calcium Carbonate CaCO3 Powder ExCal® calcium carbonate is processed from a high-purity stone, to exacting specifications at the Excalibar Minerals plants. It is suitable for use in plastics, adhesives, sealants, and other appli.. |
|||
Bulk Density | 1.12 g/cc | 0.0405 lb/in³ | |
DuPont™ Nomex® 418 Paper, 10 mil Nominal Thickness Nomex® Type 418 is designed for high-voltage applications such as motor conductor and coil wrap, transformer ground and layer insulation. It can be readily impregnated with varnishes. This calen.. |
|||
Bulk Density | 1.12 g/cc | 0.0405 lb/in³ | |
DuPont™ Nomex® 418 Paper, 14 mil Nominal Thickness Nomex® Type 418 is designed for high-voltage applications such as motor conductor and coil wrap, transformer ground and layer insulation. It can be readily impregnated with varnishes. This calen.. |
|||
Bulk Density | 1.12 g/cc | 0.0405 lb/in³ | Tapped |
CIMBAR RP 9410 Talc RP 9400 Series talcs are produced from ores, which provide an excellent balance of mechanical properties at an economical price, for primary use in commodity polypropylene. RP 9400 Series talcs are.. |
|||
Bulk Density | 1.12 - 1.28 g/cc | 0.0405 - 0.0463 lb/in³ | Nominal |
ATI Wah Chang Hafnium Oxide S Grade, HfO2 A white, free flowing powder.Information provided by ATI Wah ChangTypical Analysis: On Hf metal basis |