Physical Properties Metric English Comments
Bulk Density 0.880 - 0.940 g/cc
0.0318 - 0.0340 lb/in³
DIN 53466
Stanelco Bioplast® GS 2189 Biodegradable Plastic
Bioplast 2189 is a product that is optimised for sheet extrusion, injection and compression moulding. It is always biodegradable and readily compostable in thin sections, this material is useable i..