Physical Properties | Metric | English | Comments |
---|---|---|---|
Bulk Density | 0.900 - 1.10 g/cc | 0.0325 - 0.0397 lb/in³ | |
Nabaltec NABALOX® NO 102 Calcined Aluminum Oxide NABALOX® aluminum oxide has a number of advantages including low sintering temperaturewide sintering rangeflexible processinghigh sintered densities high wear and impact resistanceelectrical insula.. |
|||
Bulk Density | 0.900 g/cc | 0.0325 lb/in³ | |
Nabaltec APYRAL® 3 Al(OH)3 APYRAL ® from Nabaltec is an environmentally friendly halogen free product which is used as a flame retardant filler in a wide variety of rubber and polymeric materials. During thermal decompositio.. |
|||
Bulk Density | 0.900 g/cc | 0.0325 lb/in³ | ASTM D4745 |
3M Dyneon™ CC146/S Custom Fluoropolymer Compound
(discontinued **) This compound consists of a mixture of 60% bronze blended with PTFE.Information provided by Dyneon, A 3M Company |
|||
Bulk Density | 0.900 - 1.10 g/cc | 0.0325 - 0.0397 lb/in³ | |
Magyar Aluminum ALO-P90 Alumina Alumina for Polishing |
|||
Bulk Density | 0.900 g/cc | 0.0325 lb/in³ | ISO 60 |
Lanxess Pocan® DP 7318 000000 PBT, 17% Pigment PBT, 17% white pigments, injection molding, improved light reflection, low tendency to warpInformation provided by LANXESS. |
|||
Bulk Density | 0.900 - 1.20 g/cc | 0.0325 - 0.0434 lb/in³ | |
Solvay Chemicals Oxyper® S131 Sodium Percarbonate Oxyper® S131 is a stabilized grade of sodium percarbonate (Sodium carbonate peroxyhydrate) specially designed for use in bleach additive products and environmental applications; it may be suitabl.. |
|||
Bulk Density | 0.900 - 1.20 g/cc | 0.0325 - 0.0434 lb/in³ | |
Solvay Chemicals Oxyper® S142 Sodium Percarbonate Oxyper® S142 is a stabilized grade of sodium percarbonate (Sodium carbonate peroxyhydrate) specially designed for use in formulated bleach additive products, detergent powders and tablets, automa.. |
|||
Bulk Density | 0.900 - 1.20 g/cc | 0.0325 - 0.0434 lb/in³ | |
Solvay Chemicals Oxyper® SHC Sodium Percarbonate Oxyper® SHC is a high coated, stabilized grade of sodium percarbonate (Sodium carbonate peroxyhydrate) specially designed for use in bleach additive products, detergent powders and tablets, autom.. |
|||
Bulk Density | 0.900 g/cc | 0.0325 lb/in³ | |
Sharadaa Ceramics HFI Insulation Brick Services Offered: Retrofitting of Furnace, Installation of Castables/Bricks/Ceramic Fiber Modules, Castable Laying by Vibrocasting/Guiniting, Turnkey Installation Boiler/Chimney/Heater/Reformer/Rota.. |
|||
Bulk Density | 0.900 g/cc | 0.0325 lb/in³ | Dried at 110°C |
Sharadaa Ceramics REFINSUL 8S Insulating Castables Medium/High Purity Description: We offer our clients Insulating Castables that are available in medium as well as high purity. Widely used in various industries, these are renowned for their strength and heat resistan.. |
|||
Bulk Density | 0.900 g/cc | 0.0325 lb/in³ | Powder Density; ASTM D1895 |
Sumitomo Bakelite North America E 8398 Hardware Grade Epoxy Fiberglass and mineral reinforced epoxy molding compound with excellent dimensional stability, good electrical insulation properties, and good strength.Information provided by Vyncolit, a Sumitomo B.. |
|||
Bulk Density | 0.900 g/cc | 0.0325 lb/in³ | ASTM D1895 |
Sumitomo Bakelite North America E 8701A Short Glass Fiber Reinforced Epoxy E 8701A is a fiberglass and mineral reinforced epoxy molding compound, with excellent dimensional stability and good strength at elevated temperatures.Information provided by Sumitomo Bak North Amer.. |
|||
Bulk Density | 0.900 g/cc | 0.0325 lb/in³ | ASTM D1895 |
Sumitomo Bakelite North America Epiall® 1904B-1 Short Glass Fiber Reinforced Epoxy Epiall 1904B-1 is a short fiberglass reinforced epoxy molding compound, with excellent dimensional stability, good strength properties and good electrical insulation properties.Information provided .. |
|||
Bulk Density | 0.900 g/cc | 0.0325 lb/in³ | ASTM D1895 |
Sumitomo Bakelite North America Epiall® 1908-1 Short Glass Fiber Reinforced Epoxy Epiall 1908-1 is a short fiberglass reinforced epoxy molding compound, with excellent dimensional stability, good strength properties and good electrical insulation proper-ties that meets the requir.. |
|||
Bulk Density | <= 0.900 g/cc | <= 0.0325 lb/in³ | Dried at 110°C |
Sharadaa Ceramics REFINSUL ZAP-015 Insulating Castables Description: We provide our clients a range of Insulating Castables, that are used as backup layer in process industries and hot face layer in petrochemical industry. These castables are known for l.. |
|||
Bulk Density | 0.900 g/cc | 0.0325 lb/in³ | ASTM D1895 |
Sumitomo Bakelite North America SI 9550 Silicone Compound SI 9550 is a short fiberglass reinforced silicone molding compound, which offers moderate strength properties, and dimensional stability and excellent long-term thermal stability at elevated tempera.. |
|||
Bulk Density | 0.900 g/cc | 0.0325 lb/in³ | Tap |
TIMCAL TIMREX® FC250-1500 Coke TIMREX Petroleum Coke is calcined at appropriate temperature with low ash and sulfur (sulphur) content, well defined texture and consistent particle size distribution.Advantages and applications: S.. |
|||
Bulk Density | 0.900 g/cc | 0.0325 lb/in³ | Size D (tapped) |
Vesta Ceramics SicoMill® Grade 2 Silicon Powder General Description:SicoMill® is a fine-grained silicon powder, specially developed for the ceramic industry. We have five standard grinding grades, but we can produce powders adapted to single cu.. |
|||
Bulk Density | 0.900 g/cc | 0.0325 lb/in³ | Size D (tapped) |
Vesta Ceramics SicoMill® Grade 4 Silicon Powder General Description:SicoMill® is a fine-grained silicon powder, specially developed for the ceramic industry. We have five standard grinding grades, but we can produce powders adapted to single cu.. |
|||
Bulk Density | 0.900 g/cc | 0.0325 lb/in³ | ISO 60 |
Vyncolit TX10916 Graphite Filled Novolac Phenolic Novolac resin based, graphite filled compound used for low friction applications where dimensional stability is required.Information provided by Sumitomo Bak North America, Inc. |
|||
Bulk Density | 0.900 g/cc | 0.0325 lb/in³ | |
A. Schulman POLYBATCH™ White B8750A Concentrate Based In HDPE DescriptionPOLYBATCH® B8750A is a specialty white masterbatch based in HDPE. This product has been designed to achieve optimum dispersion and excellent letdown mixing in blow molding applications... |
|||
Bulk Density | >= 0.900 g/cc | >= 0.0325 lb/in³ | |
Chosun Refractories LW-30 Special Insulating Firebrick Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Bulk Density | 0.900 g/cc | 0.0325 lb/in³ | |
BASF Sicotan® Brown K 2611 Color Additive Chemical Structure: Mn/Sb/Ti-oxideApplication: Colourant for plastics; PVC-p, PVC-u, LD-PE, HD-PE, PP, PS, SB, SAN, ABS/ASA, PMMA, PC, PA, PETP, CA/CAB and UPRecommendations for food applications: B.. |
|||
Bulk Density | 0.900 g/cc | 0.0325 lb/in³ | |
BASF Sicotan® Brown K 2711 Color Additive Chemical Structure: Mn/Sb/Ti-oxideApplication: Colourant for plastics; PVC-p, PVC-u, LD-PE, HD-PE, PP, PS, SB, SAN, ABS/ASA, PMMA, PC, PA, PETP, CA/CAB and UPRecommendations for food applications: B.. |
|||
Bulk Density | 0.900 g/cc | 0.0325 lb/in³ | |
BASF Sicotan® Yellow K 1010 Color Additive Chemical Structure: Ni/Sb/Ti-oxideApplication: Colourant for plastics; PVC-p, PVC-u, LD-PE, HD-PE, PP, PS, SB, SAN, ABS/ASA, PMMA, PC, PA, PETP, CA/CAB and UPRecommendations for food applications: B.. |
|||
Bulk Density | 0.900 g/cc | 0.0325 lb/in³ | ASTM D1895 |
Plenco 1510 Polyester, Granular, Transfer Molded PLENCO 01510 is a mineral filled, pelletized polyester molding compound, which offers an excellent combination of electrical properties and dimensional stability. UL recognized under component file .. |
|||
Bulk Density | 0.900 g/cc | 0.0325 lb/in³ | ASTM D1895 |
Sumitomo Bakelite North America Epiall® 1908M-1 Short Glass Fiber Reinforced Epoxy Epiall 1908M-1 is a short glass fiber reinforced epoxy molding compound with excellent dimensional stability, good strength properties, and good electrical insulation properties.Information provided.. |
|||
Bulk Density | 0.900 g/cc | 0.0325 lb/in³ | ASTM D1895 |
Sumitomo Bakelite North America Epiall® 1961B-1 Mineral and Glass Filled Electrical Encapsulation Grade Epoxy Epiall 1961B-1 is a short glass fiber and mineral filled epoxy molding compound with excellent dimensional stability, good strength properties, and good electrical insulation properties.Information .. |
|||
Bulk Density | 0.900 g/cc | 0.0325 lb/in³ | Powder Density; ASTM D1895 |
Sumitomo Bakelite North America SI 9002J-1 Silicone Compound SI 9002J-1 is a short fiberglass reinforced silicone molding compound, which offers moderate strength properties, and dimensional stability and excellent long-term thermal stability at elevated temp.. |