Physical Properties | Metric | English | Comments |
---|---|---|---|
Bulk Density | 0.640 g/cc | 0.0231 lb/in³ | Loose |
Nyco 400 WOLLASTOCOAT® Wollastonite This grade is recommended for polymer reinforcement.Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctive particle morphology make.. |
|||
Bulk Density | 0.640 g/cc | 0.0231 lb/in³ | |
Nabaltec APYRAL® 32 Al(OH)3 APYRAL ® from Nabaltec is an environmentally friendly halogen free product which is used as a flame retardant filler in a wide variety of rubber and polymeric materials. During thermal decompositio.. |
|||
Bulk Density | 0.640 g/cc | 0.0231 lb/in³ | ASTM D1895 |
Plenco 2311 Phenolic, Granular, Injection Molded PLENCO 02311 is a versatile general purpose organic filled phenolic molding compound offering excellent mold processability and optimized cure cycles. PLENCO 02311 is also granulated to provide impr.. |
|||
Bulk Density | 0.640 g/cc | 0.0231 lb/in³ | ASTM D1895 |
Plenco 3509 Phenolic, Granular, Transfer Molded PLENCO 03509 is a mineral and flock filled phenolic molding compound offering excellent electrical properties, dimensional stability, and improved heat resistance. UL recognized under component file.. |
|||
Bulk Density | 0.640 g/cc | 0.0231 lb/in³ | ASTM D1895 |
Plenco 3557 Phenolic, Granular, Compression Molded PLENCO 03557 is a woodflour and mineral filled phenolic molding compound offering excellent dielectric strength values at elevated temperatures while maintaining mechanical strength properties. UL r.. |
|||
Bulk Density | 0.640 g/cc | 0.0231 lb/in³ | Tap |
TIMCAL TIMREX® T800 Primary Synthetic Graphite TIMREX Primary Synthetic Graphite is produced in a unique highly controlled graphitization process which assures narrow specifications and unequalled consistent quality due to: monitoring of all pro.. |
|||
Bulk Density | 0.640 g/cc | 0.0231 lb/in³ | ISO 60 |
Vyncolit X7012 Glass Fiber Reinforced Novolac Phenolic Novolac resin based, glass fiber and glass beads reinforced. High mechanical strength even at high temperatures in Long Life CoolantsInformation provided by Sumitomo Bak North America, Inc. |
|||
Bulk Density | 0.640 g/cc | 0.0231 lb/in³ | |
Zircar Ceramics IB-100B Alumina Bubble Thin wall aluminum oxide ceramic spheres offered in 2 standard bubble sizes. These low density sintered ceramic bodies are useful in a range of refractory applications with temperatures to 2000°C (.. |
|||
Bulk Density | 0.640 g/cc | 0.0231 lb/in³ | ASTM D1895 |
Plenco 2571 Phenolic, Granular, Injection Molded PLENCO 02571 is a general purpose, organic filled phenolic molding compound offering optimum cure characteristics while maintaining excellent mechanical and electrical properties. UL recognized unde.. |
|||
Bulk Density | 0.640 g/cc | 0.0231 lb/in³ | ASTM D1895 |
Plenco 4309 Phenolic, Nodular, Injection Molded PLENCO 04309 is a heat resistant, glass reinforced phenolic molding compound offering improved mechanical strength and electrical strength properties. UL recognized under component file E40654. 0430.. |
|||
Bulk Density | 0.640 g/cc | 0.0231 lb/in³ | ASTM D1895 |
Plenco 4504 Phenolic, Granular, Injection Molded Plenco 04504 is a renumber of Plaslok 504. Plenco 04504 is a two-stage, mineral and cellulose-filled phenolic molding compound having better impact and heat resistance than general purpose molding c.. |
|||
Bulk Density | 0.640 g/cc | 0.0231 lb/in³ | pellets; ISO 60 |
Covestro Makrolon® 1881 Polycarbonate Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• Impact modified• Imp.. |
|||
Bulk Density | 0.640 g/cc | 0.0231 lb/in³ | pellets; ISO 60 |
Covestro Makrolon® 1952 Polycarbonate Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• Flame retardancy• Me.. |
|||
Bulk Density | 0.640 g/cc | 0.0231 lb/in³ | pellets; ISO 60 |
Covestro Makrolon® 2405 MAS056 Polycarbonate Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• General purpose• Low.. |
|||
Bulk Density | 0.640 g/cc | 0.0231 lb/in³ | pellets; ISO 60 |
Covestro Makrolon® 2407 MAS056 Polycarbonate Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• Improved impact streng.. |
|||
Bulk Density | 0.640 g/cc | 0.0231 lb/in³ | pellets; ISO 60 |
Covestro Makrolon® 2665 Polycarbonate Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• Medium viscosity, easy.. |
|||
Bulk Density | 0.640 g/cc | 0.0231 lb/in³ | pellets; ISO 60 |
Covestro Makrolon® 6165 X Polycarbonate Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• Flame retardant• Low.. |
|||
Bulk Density | 0.640 g/cc | 0.0231 lb/in³ | pellets; ISO 60 |
Covestro Makrolon® 6255 Polycarbonate Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• Flame retardancy• Lo.. |
|||
Bulk Density | 0.640 g/cc | 0.0231 lb/in³ | |
BASF Styropor® BF 422 EPS Description: Modified expandable polystyrene (EPS) containing approximately 6 wt% pentane as the blowing agent. Styropor BF products are compatible with many anti-stat, mineral oil and color additiv.. |
|||
Bulk Density | 0.640 g/cc | 0.0231 lb/in³ | |
BASF Styropor® BFL 222 EPS Description: Modified expandable polystyrene (EPS) containing approximately 3.75 – 3.95 wt% pentane as the blowing agent. Styropor BFL products are compatible with many anti-stat, mineral oil and c.. |
|||
Bulk Density | 0.640 g/cc | 0.0231 lb/in³ | |
BASF Styropor® BFL 322 EPS Description: Modified expandable polystyrene (EPS) containing approximately 3.75 – 3.95 wt% pentane as the blowing agent. Styropor BFL products are compatible with many anti-stat, mineral oil and c.. |
|||
Bulk Density | 0.640 g/cc | 0.0231 lb/in³ | |
BASF Styropor® BFL 327 EPS Description: Modified expandable polystyrene (EPS) containing approximately 3.75 – 3.95 wt% pentane as the blowing agent. Styropor BFL products are compatible with many anti-stat, mineral oil and c.. |
|||
Bulk Density | 0.640 - 0.740 g/cc | 0.0231 - 0.0267 lb/in³ | |
BASF Ultramid® B36 LNV PA6 Information provided by BASF |
|||
Bulk Density | 0.640 - 0.740 g/cc | 0.0231 - 0.0267 lb/in³ | |
BASF Ultramid® B40 L PA6 Description: Ultramid® B40 L is a lubricated polyamide 6 grade of high viscosity that is well suited for the production of blown and cast film and monofilaments. Product supplied in 2-2.5 mm round .. |
|||
Bulk Density | 0.640 - 0.740 g/cc | 0.0231 - 0.0267 lb/in³ | |
BASF Ultramid® B40 LN PA6 Description: Ultramid® B40 LN is a polyamide 6 grade of high viscosity that is well suited for the production of blown and cast film. Clarity and thermoformability are enhanced by the incorporation.. |
|||
Bulk Density | 0.640 - 0.740 g/cc | 0.0231 - 0.0267 lb/in³ | |
BASF Ultramid® B27 SD 02 PA6 Description: Ultramid® B27 SD 02 is a polyamide 6 for the production of semi dull textile and carpet fibers. Product comes in 2-2.5 mm cylindrical pellets.Information provided by BASF |
|||
Bulk Density | 0.640 - 0.740 g/cc | 0.0231 - 0.0267 lb/in³ | |
BASF Ultramid® B33 L PA6 Description: Ultramid® B33 L is a lubricated polyamide 6 grade of intermediate viscosity that is well suited for the production of biaxial oriented and cast film and monofilaments. Product comes .. |
|||
Bulk Density | 0.640 g/cc | 0.0231 lb/in³ | |
BASF Styropor® BF 322 EPS Description: Modified expandable polystyrene (EPS) containing approximately 6 wt% pentane as the blowing agent. Styropor BF products are compatible with many anti-stat, mineral oil and color additiv.. |
|||
Bulk Density | 0.640 - 0.740 g/cc | 0.0231 - 0.0267 lb/in³ | |
BASF Ultramid® B36 LN 01 PA6 Description: Ultramid® B36 LN 01 is a polyamide 6 grade of intermediate to high viscosity that is well suited for the production of cast and blown film. Clarity and thermoformability are enhanced b.. |