Physical Properties | Metric | English | Comments |
---|---|---|---|
Bulk Density | 0.310 - 0.410 g/cc | 0.0112 - 0.0148 lb/in³ | ASTM D1895 |
LG Chemical PB1120 PVC General Description: PB1120, homopolymer made by micro-suspension seeded polymerization, is medium-viscosity PVC resin with pseudo plastic flow property. It can be used for foam flooring layer and w.. |
|||
Bulk Density | 0.310 - 0.410 g/cc | 0.0112 - 0.0148 lb/in³ | ASTM D1895 |
LG Chemical PB1202 PVC General Description: PB1202, homopolymer made by micro-suspension seeded polymerization, PVC Resin has a fluid property similar to Newtonian fluidity (low-viscosity) It is mainly used for non-foamin.. |
|||
Bulk Density | 0.310 - 0.410 g/cc | 0.0112 - 0.0148 lb/in³ | ASTM D1895 |
LG Chemical PB1302 PVC General Description: PB1302, homopolymer made from micro-suspension seeded polymerization, is a low-viscosity PVC resin with a pseudo-plastic flow property in processing range. It can be used for ca.. |
|||
Bulk Density | 0.310 - 0.410 g/cc | 0.0112 - 0.0148 lb/in³ | ASTM D1895 |
LG Chemical PE1311 PVC General Description: PE1311, homopolymer made by emulsion polymerization, is a high-viscosity PVC resin with pseudo-plastic flow property PE1311 has an good chemical foaming with low density and fin.. |