Physical Properties | Metric | English | Comments |
---|---|---|---|
Bulk Density | 0.272 g/cc | 0.00983 lb/in³ | |
PolyOne Geon™ 170 Series 171 Polyvinyl Chloride Homopolymer (PVC Homopolymer) Geon® 171 is an ultra-high molecular weight, fine particle size homopolymer dispersion resin intended for use in thin, organosol cast coatings and films. This resin provides excellent fused film an.. |
|||
Bulk Density | 0.272 g/cc | 0.00983 lb/in³ | |
PolyOne Geon™ 170 Series 178 Polyvinyl Chloride Homopolymer (PVC Homopolymer) Geon® 178 is a high molecular weight, fine particle size homopolymer dispersion resin. It provides the ability to produce thin gauge coatings. It is recommended for applications such as food and be.. |
|||
Bulk Density | 0.272 g/cc | 0.00983 lb/in³ | |
PolyOne Geon™ 170 Series 4195 Polyvinyl Chloride Homopolymer (PVC Homopolymer) Geon® 171 is an ultra-high molecular weight, fine particle size homopolymer dispersion resin intended for use in thin, organosol cast coatings and films. This resin provides excellent fused film an.. |
|||
Bulk Density | 0.272 g/cc | 0.00983 lb/in³ | |
PolyOne Geon™ 170 Series Adept E 49 Polyvinyl Chloride Homopolymer (PVC Homopolymer) Geon® Adept E49 is a low molecular weight homopolymer dispersion resins intended for use in variety of plastisol applications and processes. It reduces scrap rates and manufacturing costs by extend.. |
|||
Bulk Density | 0.272 g/cc | 0.00983 lb/in³ | |
PolyOne Geon™ 170 Series L100UF Polyvinyl Chloride Homopolymer (PVC Homopolymer) Geon® Ultrafine 170-L100UF is a medium molecular weight, ultrafine particle size homopolymer dispersion resin. With the very fine particle size, it provides excellent casting characteristics for th.. |
|||
Bulk Density | 0.272 g/cc | 0.00983 lb/in³ | |
PolyOne Geon™ 170 Series L120UF Polyvinyl Chloride Homopolymer (PVC Homopolymer) Geon® Ultrafine 170-L120UF is a high molecular weight, ultrafine particle size homopolymer dispersion resin. With the very fine particle size, it provides excellent casting characteristics for thin.. |
|||
Bulk Density | 0.272 g/cc | 0.00983 lb/in³ | |
PolyOne Geon™ 170 Series L140UF Polyvinyl Chloride Homopolymer (PVC Homopolymer) Geon® Ultrafine 170-L140UF is an ultra high molecular weight, ultrafine particle size homopolymer dispersion resin. The excellent dispersibility provides good product throughput during the organoso.. |
|||
Bulk Density | 0.272 g/cc | 0.00983 lb/in³ | |
PolyOne Geon™ 170 Series 174 Polyvinyl Chloride Homopolymer (PVC Homopolymer) Geon® 174 is a medium molecular weight, fine particle size homopolymer dispersion resin. It provides a good balance of fused film properties and processing temperatures. It is recommended for appli.. |
|||
Bulk Density | 0.272 - 0.288 g/cc | 0.00984 - 0.0104 lb/in³ | Loose |
KaMin Polyplate® P01 Kaolin Clay - Delaminated Polyplate® P01 is a milled, high brightness, large particle size delaminated kaolin, intended for use in solvent and water-borne coatings, inks, and adhesives. The high aspect ratio of the large .. |