Physical Properties | Metric | English | Comments |
---|---|---|---|
Bulk Density | 0.260 g/cc | 0.00939 lb/in³ | |
Potters Industries Q-Cel® 6042S Performance Benefits: A low-density, performance-enhancing additive.Fewer defects: excellent mold flow, uniform dispersionReduced compound density and viscosityIncreased acoustic and thermal insulat.. |
|||
Bulk Density | 0.260 g/cc | 0.00937 lb/in³ | |
Potters Industries Q-Cel® 7040S Hollow Engineered Glass Microspheres Q-CEL® hollow glass microspheres are alternatives to conventional fillers and additives such as silicas, calcium carbonates, talc, clay, etc. A variety of particle sizes, densities and strengths me.. |
|||
Bulk Density | 0.260 g/cc | 0.00937 lb/in³ | |
Potters Industries Sphericel® 45P25 Hollow Engineered Glass Microspheres Sphericel® hollow glass microspheres are alternatives to conventional fillers and additives such as silicas, calcium carbonates, talc, clay, etc. A variety of particle sizes, densities and strength.. |
|||
Bulk Density | 0.260 g/cc | 0.00939 lb/in³ | Tap Density |
Momentive Performance Materials AC6069 Boron Nitride (BN) Powder GE Advanced Ceramics boron nitride (BN) powder grade AC6069 consists of single-crystal hexagonal particles with an average particle size of 9 µm. AC6069 has a relatively tight particle size distr.. |
|||
Bulk Density | 0.260 g/cc | 0.00939 lb/in³ | |
Zircar Ceramics AXHTM Alumina-Silica Insulation ZIRCAR Alumina Silica Insulation Type AXL and Type AXHTM are inorganically bound insulation boards typified by their rigid outer surfaces and unbound interiors. They offer low thermal conductivity a.. |
|||
Bulk Density | 0.260 g/cc | 0.00937 lb/in³ | |
BNZ Materials Zelieblok 2000S Structural Ceramic Insulation Information provided by BNZ Materials Inc. |
|||
Bulk Density | >= 0.260 g/cc | >= 0.00939 lb/in³ | |
Oceanchem Group Magnesium Hydroxide Molecular Formula: Mg(OH)2Cas No.: 1309-42-8Use: Magnesium hydroxide is a non-halogen flame retardant recommended where use of halogenated products is limited or prohibited. In addition, it is an e.. |