Physical Properties Metric English Comments
Bulk Density 0.0800 g/cc
0.00289 lb/in³
Shipping
Zircar Zirconia BusterF Alumina Bulk Fiber Insulation
Alumina Bulk Fibers Type BusterF are Hi-Alpha alumina fibers available in two different forms, both having useful properties up to 1700°C. These polycrystalline fibers can be vacuum formed into rig..
Bulk Density 0.0800 g/cc
0.00289 lb/in³
Inhance Fluoro-Seal INHANCE® KF Aramid Fiber Pulp
Product Description: INHANCE KF fiber is an aramid fiber pulp that has been surface activated by a proprietary reactive gas process. Surface activation makes the fibers easy to disperse, and create..
Bulk Density 0.0800 g/cc
0.00289 lb/in³
Scott
TIMCAL TIMREX® LSG10 Natural Graphite
TIMREX Natural Flake Graphite is produced in a wide range of products distinguished by particle size distribution, chemistry and carbon content. Timcal mines the graphite from its own source in Lac-..
Bulk Density 0.0800 g/cc
0.00289 lb/in³
Scott, Typical
TIMCAL TIMREX® PP 25 Natural Flake Graphite
TIMREX Natural Flake Graphite is produced in a wide range of products distinguished by particle size distribution, chemistry and carbon content. Timcal mines the graphite from its own source in Lac-..
Bulk Density 0.0800 g/cc
0.00289 lb/in³
Zircar Ceramics ALBF Alumina Bulk Fiber
Alumina Bulk Fiber Type ALBF consists of long aluminum oxide fibers suited for the vacuum forming of low density shapes. The high alpha alumina content and addition of a grain growth inhibitor give ..
Bulk Density 0.0800 g/cc
0.00289 lb/in³
Shipping
Zircar Zirconia BusterF Alumina Bulk Fiber Insulation
Alumina Bulk Fibers Type BusterF are Hi-Alpha alumina fibers available in two different forms, both having useful properties up to 1700°C. These polycrystalline fibers can be vacuum formed into rig..
Bulk Density 0.0800 g/cc
0.00289 lb/in³
Scott
TIMCAL TIMREX® MX25 Primary Synthetic Graphite
TIMREX Primary Synthetic Graphite is produced in a unique highly controlled graphitization process which assures narrow specifications and unequalled consistent quality due to: monitoring of all pro..
Bulk Density 0.0800 g/cc
0.00289 lb/in³
of Dry Beads
Mo-Sci Corporation GL-0237 Hollow Glass Spheres
Appearance: Hollow microspheres with white color in powder form.Applications: GL-0237 is a new, low cost, light weight, hollow glass extender for liquid resin systems offering low cost per unit volu..
Bulk Density 0.0800 g/cc
0.00289 lb/in³
Potters Industries Q-Cel® 6014
Performance Benefits: A low-density, performance-enhancing additive.Fewer defects: excellent mold flow, uniform dispersionReduced compound density and viscosityIncreased acoustic and thermal insulat..