Physical Properties Metric English Comments
Bulk Density 1.12 g/cc
0.0405 lb/in³
Tapped
Nyco NYAD G® WOLLASTOCOAT® Wollastonite
Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctive particle morphology makes wollastonite an ideal performance mineral for a br..
Bulk Density 1.12 g/cc
0.0405 lb/in³
packed
Imerys Minsparâ„¢ 200 Feldspar
Minspar 200 is 200 mesh flotation grade soda Feldspar used in the ceramic whiteware industry for sanitaryware, dinnerware, floor and wall tile, artware and glazes.Information provided by Imerys
Bulk Density 1.12 g/cc
0.0405 lb/in³
packed
Imerys Minsparâ„¢ 3 Ground Feldspar
Minsparâ„¢ 3 is a coarse particle size, ground Feldspar with a tightly controlled particle size distribution. The angular particle shape and inherent cheMical resistance make Minsparâ„¢ 3 an e..
Bulk Density 1.12 g/cc
0.0405 lb/in³
Standard
GrafTech GRAFIHX® RXS Series Flexible Graphite Heat Transfer Plates
GRAFIHX® RXS Series are heat transfer plates for radiant heating applications made from high thermal conductivity flexible graphite. They are available in rolls and sheets as a replacement for tr..
Bulk Density 1.12 g/cc
0.0405 lb/in³
Available
GrafTech GRAFOIL® GHC Standard Internal Combustion Laminate
GRAFOIL® Grade GHC is a laminate made from Grade GTC flexible graphite. Laminate Construction: GRAFOIL® Grade GTC ? Micro-thin, phenolic-based adhesive ? GRAFOIL® Grade GTC
Bulk Density 1.12 g/cc
0.0405 lb/in³
Standard; Graphite
GrafTech GRAFOIL® GHE Standard Fluid Sealing Laminate, Metal Reinforced
GRAFOIL® Grade GHE laminate is made with GTB flexible graphite mechanically bonded to both faces of a 316 or 316L stainless steel tang metal insert. Surface identifiable, the laminate is branded ..
Bulk Density 1.12 g/cc
0.0405 lb/in³
Standard; Graphite
GrafTech GRAFOIL® GHH Standard Internal Combustion Laminate, Metal Reinforced
GRAFOIL® Grade GHH is a laminate made with GRAFOIL® Grade GTC flexible graphite chemically bonded to both faces of a flat, low-carbon steel core. Its applications include: exhaust sealing, ga..
Bulk Density 1.12 g/cc
0.0405 lb/in³
Standard; Graphite
GrafTech GRAFOIL® GHJ Non-Standard Internal Combustion Grade GHJ Laminate, Metal Reinforced
GRAFOIL® Grade GHJ is a laminate made with GRAFOIL® Grade GTC flexible graphite mechanically attached to a perforated, low-carbon steel core. Its applications include: exhaust manifold gasket..
Bulk Density 1.12 g/cc
0.0405 lb/in³
Standard; Graphite
GrafTech GRAFOIL® GHL Standard Fluid Sealing Grade GHL Laminate
GRAFOIL® Grade GHL is a laminate made with GRAFOIL® Grade GTB flexible graphite. Laminate thicknesses > 0.060" will be adhesively bonded to final thickness. Laminate thicknesses
Bulk Density 1.12 g/cc
0.0405 lb/in³
Standard; Graphite
GrafTech GRAFOIL® GHR Standard Fluid Sealing Laminate, Metal Reinforced
GRAFOIL® Grade GHR is an uncured laminate made with GRAFOIL® Grade GTB flexible graphite adhesively bonded to both faces of a 0.002" thick flat 316 or 316L stainless steel insert. Surface iden..
Bulk Density 1.12 g/cc
0.0405 lb/in³
Standard; Graphite
GrafTech GRAFOIL® GHW Standard Fluid Sealing Laminate, Non-Metal Reinforced
GRAFOIL® Grade GHW is a laminate made with GRAFOIL® Grade GTB flexible graphite thermally bonded to a 0.0025" thick high-temperature continuous woven glass fiber insert. Its functional tempera..
Bulk Density 1.12 g/cc
0.0405 lb/in³
Standard
GrafTech GRAFOIL® GTA Standard Fluid Sealing Graphite Single Layer Gasketing Material
GRAFOIL® GTA premium flexible graphite is a non-inhibited grade developed for use in nuclear or semiconductor applications. It is certified to meet the most rigorous purity specifications of the ..
Bulk Density 1.12 g/cc
0.0405 lb/in³
Standard for 0.005", 0.010", 0.015", 0.020", 0.025", 0.030", 0.060" thick
GrafTech GRAFOIL® GTB Standard Fluid Sealing Graphite Single Layer Gasketing Material
GRAFOIL® GTB flexible graphite sheet is a gasketing material containing no binders or fillers. Standard industrial grade GTB flexible graphite has an oxidation/corrosion inhibitor and is typicall..
Bulk Density 1.12 g/cc
0.0405 lb/in³
Standard
GrafTech GRAFOIL® GTC Standard Internal Combustion Graphite, Single Layer Material
GRAFOIL® GTC flexible graphite sheet is a gasketing material containing no binders or fillers, which will seal a wide variety of liquids and gases over an extremely large temperature range. GTC c..
Bulk Density 1.12 g/cc
0.0405 lb/in³
Standard; Graphite
GrafTech GRAFOIL® GTH Standard Fluid Sealing Adhesive-Backed Tape, Gasket and Thread Tape
GRAFOIL® Grade GTH is a pressure sensitive adhesive-backed tape made with GRAFOIL® Grade GTB flexible graphite. It applications include: threaded joints, forming place gaskets, and large diam..
Bulk Density 1.12 g/cc
0.0405 lb/in³
Standard
GrafTech GRAFOIL® GTJ Standard Fluid Sealing Graphite, Single Layer Material
GRAFOIL® GTJ premium flexible graphite is an oxidation/corrosion inhibited grade developed for use in nuclear and high temp, high purity applications. It is certified to meet the most rigorous pu..
Bulk Density 1.12 g/cc
0.0405 lb/in³
Standard
GrafTech GRAFOIL® GTX Standard Fluid Sealing Graphite, Single Layer Material
GRAFOIL® GTX flexible graphite sheet is inhibited for high oxidation/corrosion resistance that can be used for most fluid sealing and industrial applications. Grade GTX contains an inorganic, non..
Bulk Density 1.12 g/cc
0.0405 lb/in³
Standard
GrafTech GRAFOIL® SUPER GTO® Standard Internal Combustion Single Layer Gasketing Material
GRAFOIL® SUPER GTO® flexible graphite sheet is a gasketing material containing no binders, which will seal a wide variety of liquids and gases over an extremely large temperature range (-240Â..
Bulk Density 1.12 g/cc
0.0405 lb/in³
Standard; Graphite
GrafTech GRAFOIL® TG-251 Standard Internal Combustion Laminate, Metal Reinforced
GRAFOIL® Grade TG-251 is GRAFOIL® Grade GTC flexible graphite chemically bonded to both faces of a flat, low-carbon steel core. Its applications include: exhaust sealing, gasoline/diesel head..
Bulk Density 1.12 g/cc
0.0405 lb/in³
Available
GrafTech GRAFOIL® TG-411 Non-Standard Fluid Sealing Graphite, High Temperature
GRAFOIL® TG-411 is a high temperature purified flexible graphite sheet for applications that require extremely low impurity levels. Material greater than 0.040" (1 mm) thick is adhesively bonded ..
Bulk Density 1.12 g/cc
0.0405 lb/in³
Standard; Graphite
GrafTech GRAFOIL® GRAFKOTE® Laminates, Non-Metal Reinforced
GRAFOIL® GRAFKOTE® laminates are made with GRAFOIL® Grade GTB flexible graphite thermally bonded to a 0.0005" thick polymer facing on one ("Single-Sided") or both ("Double-Sided") sides. Th..
Bulk Density 1.12 g/cc
0.0405 lb/in³
Packed
Excalibar ExCal® 400 Calcium Carbonate CaCO3 Powder
ExCal® calcium carbonate is processed from a high-purity stone, to exacting specifications at the Excalibar Minerals plants. It is suitable for use in plastics, adhesives, sealants, and other appli..
Bulk Density 1.12 g/cc
0.0405 lb/in³
DuPont™ Nomex® 418 Paper, 10 mil Nominal Thickness
Nomex® Type 418 is designed for high-voltage applications such as motor conductor and coil wrap, transformer ground and layer insulation. It can be readily impregnated with varnishes. This calen..
Bulk Density 1.12 g/cc
0.0405 lb/in³
DuPont™ Nomex® 418 Paper, 14 mil Nominal Thickness
Nomex® Type 418 is designed for high-voltage applications such as motor conductor and coil wrap, transformer ground and layer insulation. It can be readily impregnated with varnishes. This calen..
Bulk Density 1.12 g/cc
0.0405 lb/in³
Tapped
CIMBAR RP 9410 Talc
RP 9400 Series talcs are produced from ores, which provide an excellent balance of mechanical properties at an economical price, for primary use in commodity polypropylene. RP 9400 Series talcs are..
Bulk Density 1.12 - 1.28 g/cc
0.0405 - 0.0463 lb/in³
Nominal
ATI Wah Chang Hafnium Oxide S Grade, HfO2
A white, free flowing powder.Information provided by ATI Wah ChangTypical Analysis: On Hf metal basis