Physical Properties Metric English Comments
Bulk Density 1.00 - 1.10 g/cc
0.0361 - 0.0397 lb/in³
Nabaltec GRANALOX® NM 9922 I Ceramic Bodies
Nabaltec`s GRANALOX® Ceramic bodies are produced under rigid quality control of green and sintered density, shrinkage, porosity, loss on ignition and granulate size. The properties of the corundum ..
Bulk Density 0.900 - 1.10 g/cc
0.0325 - 0.0397 lb/in³
Nabaltec NABALOX® NO 102 Calcined Aluminum Oxide
NABALOX® aluminum oxide has a number of advantages including low sintering temperaturewide sintering rangeflexible processinghigh sintered densities high wear and impact resistanceelectrical insula..
Bulk Density 0.900 - 1.10 g/cc
0.0325 - 0.0397 lb/in³
Nabaltec NABALOX® NO 103 Calcined Aluminum Oxide
NABALOX® aluminum oxide has a number of advantages including low sintering temperaturewide sintering rangeflexible processinghigh sintered densities high wear and impact resistanceelectrical insula..
Bulk Density 0.900 - 1.10 g/cc
0.0325 - 0.0397 lb/in³
Magyar Aluminum ALO-B15 Alumina
Calcined Alumina; Minimum 5% alpha-Al2O3.
Bulk Density 0.800 - 1.10 g/cc
0.0289 - 0.0397 lb/in³
Magyar Aluminum ALO-DFC Alumina
Alumina for Polishing
Bulk Density 0.900 - 1.10 g/cc
0.0325 - 0.0397 lb/in³
Magyar Aluminum ALO-P90 Alumina
Alumina for Polishing
Bulk Density 1.00 - 1.10 g/cc
0.0361 - 0.0397 lb/in³
After drying at 110°C
Gouda Vuurvast GOLITE 1.2.4. Mix Refractory Insulating Castable
Description: This lightweight castable is composed of 1 part cement, 2 parts light weight grains and 4 parts vermiculite. Special additives provide for higher strength and less shrinkage.Remarks: Th..
Bulk Density 1.00 - 1.10 g/cc
0.0361 - 0.0397 lb/in³
After drying at 110°C
Gouda Vuurvast GOLITE 135 L Refractory Insulating Castable
Description: Golite 135 L can be used in direct contact with fire and combines a good strength with a high insulation value.Remarks: These values apply to cast products. Also available in gunning va..