Physical Properties | Metric | English | Comments |
---|---|---|---|
Bulk Density | 0.0300 - 0.0360 g/cc | 0.00108 - 0.00130 lb/in³ | |
BASF Neopolen® P 9035 0.035 g/cc Core density; Expanded Polypropylene (Europe) Description: Neopolen® P 9035 is expanded Polypropylene supplied in the form of beads. The cells are largely closed.Physical properties of moldings made from Neopolen® P 9035.Note: In order to mea.. |
|||
Bulk Density | 0.0300 - 0.0360 g/cc | 0.00108 - 0.00130 lb/in³ | |
BASF Neopolen® P 9035 0.04 g/cc Core density; Expanded Polypropylene (Europe) Description: Neopolen® P 9035 is expanded Polypropylene supplied in the form of beads. The cells are largely closed.Physical properties of moldings made from Neopolen® P 9035.Note: In order to mea.. |
|||
Bulk Density | 0.0300 - 0.0360 g/cc | 0.00108 - 0.00130 lb/in³ | |
BASF Neopolen® P 9035 0.05 g/cc Core density; Expanded Polypropylene (Europe) Description: Neopolen® P 9035 is expanded Polypropylene supplied in the form of beads. The cells are largely closed.Physical properties of moldings made from Neopolen® P 9035.Note: In order to mea.. |
|||
Bulk Density | 0.0300 - 0.0360 g/cc | 0.00108 - 0.00130 lb/in³ | |
BASF Neopolen® P 9035 0.06 g/cc Core density; Expanded Polypropylene (Europe) Description: Neopolen® P 9035 is expanded Polypropylene supplied in the form of beads. The cells are largely closed.Physical properties of moldings made from Neopolen® P 9035.Note: In order to mea.. |
|||
Bulk Density | 0.0300 - 0.0360 g/cc | 0.00108 - 0.00130 lb/in³ | |
BASF Neopolen® P 9035 0.07 g/cc Core density; Expanded Polypropylene (Europe) Description: Neopolen® P 9035 is expanded Polypropylene supplied in the form of beads. The cells are largely closed.Physical properties of moldings made from Neopolen® P 9035.Note: In order to mea.. |
|||
Bulk Density | 0.0300 - 0.0360 g/cc | 0.00108 - 0.00130 lb/in³ | |
BASF Neopolen® P 9235 0.04 g/cc Core density; Expanded Polypropylene (Europe) Description: Neopolen® P 9235 is expanded Polypropylene supplied in the form of beads. The cells are largely closed.Physical properties of moldings made from Neopolen® P 9235.Note: In order to mea.. |
|||
Bulk Density | 0.0300 - 0.0360 g/cc | 0.00108 - 0.00130 lb/in³ | |
BASF Neopolen® P 9435 0.04 g/cc Core density; Expanded Polypropylene (Europe) Description: Neopolen® P 9435 is expanded Polypropylene supplied in the form of beads. The cells are largely closed.Physical properties of moldings made from Neopolen® P 9435.Note: In order to mea.. |
|||
Bulk Density | 0.0300 - 0.0360 g/cc | 0.00108 - 0.00130 lb/in³ | |
BASF Neopolen® P 9435 0.05 g/cc Core density; Expanded Polypropylene (Europe) Description: Neopolen® P 9435 is expanded Polypropylene supplied in the form of beads. The cells are largely closed.Physical properties of moldings made from Neopolen® P 9435.Note: In order to mea.. |
|||
Bulk Density | 0.0300 - 0.0360 g/cc | 0.00108 - 0.00130 lb/in³ | |
BASF Neopolen® P 9435 0.06 g/cc Core density; Expanded Polypropylene (Europe) Description: Neopolen® P 9435 is expanded Polypropylene supplied in the form of beads. The cells are largely closed.Physical properties of moldings made from Neopolen® P 9435.Note: In order to mea.. |
|||
Bulk Density | 0.0300 - 0.0360 g/cc | 0.00108 - 0.00130 lb/in³ | |
BASF Neopolen® P 9235 0.035 g/cc Core density; Expanded Polypropylene (Europe) Description: Neopolen® P 9235 is expanded Polypropylene supplied in the form of beads. The cells are largely closed.Physical properties of moldings made from Neopolen® P 9235.Note: In order to mea.. |
|||
Bulk Density | 0.0300 - 0.0360 g/cc | 0.00108 - 0.00130 lb/in³ | |
BASF Neopolen® P 9235 0.05 g/cc Core density; Expanded Polypropylene (Europe) Description: Neopolen® P 9235 is expanded Polypropylene supplied in the form of beads. The cells are largely closed.Physical properties of moldings made from Neopolen® P 9235.Note: In order to mea.. |
|||
Bulk Density | 0.0300 - 0.0360 g/cc | 0.00108 - 0.00130 lb/in³ | |
BASF Neopolen® P 9235 0.06 g/cc Core density; Expanded Polypropylene (Europe) Description: Neopolen® P 9235 is expanded Polypropylene supplied in the form of beads. The cells are largely closed.Physical properties of moldings made from Neopolen® P 9235.Note: In order to mea.. |
|||
Bulk Density | 0.0300 - 0.0360 g/cc | 0.00108 - 0.00130 lb/in³ | |
BASF Neopolen® P 9235 0.07 g/cc Core density; Expanded Polypropylene (Europe) Description: Neopolen® P 9235 is expanded Polypropylene supplied in the form of beads. The cells are largely closed.Physical properties of moldings made from Neopolen® P 9235.Note: In order to mea.. |
|||
Bulk Density | 0.0300 - 0.0360 g/cc | 0.00108 - 0.00130 lb/in³ | |
BASF Neopolen® P 9435 0.07 g/cc Core density; Expanded Polypropylene (Europe) Description: Neopolen® P 9435 is expanded Polypropylene supplied in the form of beads. The cells are largely closed.Physical properties of moldings made from Neopolen® P 9435.Note: In order to mea.. |
|||
Bulk Density | 0.0300 - 0.0360 g/cc | 0.00108 - 0.00130 lb/in³ | |
BASF Neopolen® P 9435 0.035 g/cc Core density; Expanded Polypropylene (Europe) Description: Neopolen® P 9435 is expanded Polypropylene supplied in the form of beads. The cells are largely closed.Physical properties of moldings made from Neopolen® P 9435.Note: In order to mea.. |