Physical Properties | Metric | English | Comments |
---|---|---|---|
Bulk Density | 0.960 g/cc | 0.0347 lb/in³ | Tapped |
Nyco NYCOR® R Wollastonite Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctive particle morphology makes wollastonite an ideal performance mineral for a br.. |
|||
Bulk Density | 0.960 g/cc | 0.0347 lb/in³ | |
Zircar Zirconia ZYFB-6 Zirconia Boards, Discs, and Cylinders Insulation Type ZYFB Boards, Discs and Cylinders are rigid, refractory structures composed of yttria-stabilized zirconia fibers that do not undergo the usual phase transitions associated with pure zirconia. Ty.. |
|||
Bulk Density | 0.961 g/cc | 0.0347 lb/in³ | packed |
Imerys Minsparâ„¢ 4 Ground Feldspar Minsparâ„¢ 4 is a medium particle size, ground Feldspar with a tightly controlled particle size distribution. The small amount of material retained on a 325 mesh screen, in conjunction with excel.. |
|||
Bulk Density | 0.960 g/cc | 0.0347 lb/in³ | ASTM D1895 |
Sumitomo Bakelite Sumikon® PM-9610 Glass-Filled Phenolic, Compression Grade Sumikon PM-9610 is a two stage glass fiber and mineral filled black phenolic special purpose molding compound. It is especially designed for applications requiring high strength and higher dimens.. |
|||
Bulk Density | 0.960 g/cc | 0.0347 lb/in³ | ASTM D1895 |
Sumitomo Bakelite Sumikon® PM-9610 Glass-Filled Phenolic, Injection Grade Sumikon PM-9610 is a two stage glass fiber and mineral filled black phenolic special purpose molding compound. It is especially designed for applications requiring high strength and higher dimens.. |
|||
Bulk Density | 0.960 g/cc | 0.0347 lb/in³ | ASTM D1895 |
Plenco 1510 Polyester, Pellet, Injection Molded PLENCO 01510 is a mineral filled, pelletized polyester molding compound, which offers an excellent combination of electrical properties and dimensional stability. UL recognized under component file .. |
|||
Bulk Density | 0.960 g/cc | 0.0347 lb/in³ | |
Zircar Zirconia ZYFB-6 Zirconia Boards, Discs, and Cylinders Insulation Type ZYFB Boards, Discs and Cylinders are rigid, refractory structures composed of yttria-stabilized zirconia fibers that do not undergo the usual phase transitions associated with pure zirconia. Ty.. |
|||
Bulk Density | 0.960 g/cc | 0.0347 lb/in³ | |
Zircar Zirconia ZYZ-6 Zirconia Boards and Discs Insulation Type ZYZ Boards and Discs are rigid, refractory structures composed of yttria-stabilized zirconia fibers that are bonded with silica. This unique composition provides Type ZYZ insulation with the lo.. |
|||
Bulk Density | 0.961 g/cc | 0.0347 lb/in³ | Loose |
Excalibar ExBar™ W 2 Barite BaSO4 Powder ExBar™ W high-purity white barytes are manufactured using only the highest quality white, natural barium sulfate ore. Strict quality control results in consistent products that are used in paints, .. |
|||
Bulk Density | 0.961 g/cc | 0.0347 lb/in³ | Loose |
Excalibar ExCal® 200 Calcium Carbonate CaCO3 Powder ExCal® calcium carbonate is processed from a high-purity stone, to exacting specifications at the Excalibar Minerals plants. It is suitable for use in plastics, adhesives, sealants, and other appli.. |
|||
Bulk Density | 0.961 g/cc | 0.0347 lb/in³ | Tapped |
CIMBAR Gel Talc for Polyester Filler Gel Talc and Body Filler talc products are produced from high purity ore. Gel Talc and Body Filler products provide an excellent balance of color and mechanical properties for primary use in polyes.. |
|||
Bulk Density | 0.961 g/cc | 0.0347 lb/in³ | Tapped |
CIMBAR RP 9305 Talc RP 9300 Series talcs are produced from high purity ores, which provide an excellent balance of color and mechanical properties, for primary use in commodity polypropylene and polyester compounds. R.. |
|||
Bulk Density | 0.961 g/cc | 0.0347 lb/in³ | |
CIMBAR Suspengel™ 325 High Purity Bentonite, Industrial Grade Suspengel products are manufactured from the highest quality Western Bentonite reserves. Suspengel products are easy to disperse thixotropes with excellent suspension properties. Strict process co.. |
|||
Bulk Density | 0.961 g/cc | 0.0347 lb/in³ | |
Arkema Group KYNAR FLEX® 2800-01 Polyvinylidene Fluoride Copolymer - Extrusion Characteristics: Natural resin - translucent, off-white hemispheres. Flexible, lubricated. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechanical s.. |
|||
Bulk Density | 0.961 g/cc | 0.0347 lb/in³ | |
Arkema Group KYNAR FLEX® 2850-04 Polyvinylidene Fluoride Copolymer - Extrusion & Molding Characteristics: Natural resin - translucent, off-white hemispheres. 150°C Temperature rating. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechani.. |
|||
Bulk Density | 0.961 g/cc | 0.0347 lb/in³ | |
Arkema Group KYNAR FLEX® 2950-05 Polyvinylidene Fluoride Copolymer - Extrusion & Molding Characteristics: Natural resin - translucent, off-white hemispheres. Very flexible, flame and smoke suppressant. High stability in harsh thermal, chemical and ultraviolet environments. High toug.. |
|||
Bulk Density | 0.961 g/cc | 0.0347 lb/in³ | |
Arkema Group KYNAR FLEX® 3120-15 Polyvinylidene Fluoride Copolymer - Extrusion & Molding Characteristics: Natural resin - translucent, off-white hemispheres. Flexible, flame and smoke suppressant. High stability in harsh thermal, chemical and ultraviolet environments. High toughness.. |
|||
Bulk Density | 0.961 g/cc | 0.0347 lb/in³ | |
Arkema Group KYNAR FLEX® 3120-50 Polyvinylidene Fluoride Copolymer - Extrusion & Molding Characteristics: Natural resin - translucent, off-white hemispheres. Flexible, 150°C temperature rating. High stability in harsh thermal, chemical and ultraviolet environments. High toughness a.. |
|||
Bulk Density | 0.961 g/cc | 0.0347 lb/in³ | |
Arkema Group KYNAR® 710, 710 HDP Polyvinylidene Fluoride Homopolymer- Injection Molding Characteristics: Natural resin - translucent, off-white hemispheres. HDP indicates higher color stability. High stability in harsh thermal, chemical and ultraviolet environments. High toughness .. |
|||
Bulk Density | 0.961 g/cc | 0.0347 lb/in³ | |
Arkema Group KYNAR® 740 Polyvinylidene Fluoride Homopolymer - Injection Molding and Extrusion Characteristics: Natural resin - translucent, off-white hemispheres. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechanical strength, low permeabili.. |
|||
Bulk Density | 0.961 g/cc | 0.0347 lb/in³ | |
Arkema Group KYNAR® 740-02 Polyvinylidene Fluoride Homopolymer - Injection Molding and Extrusion Characteristics: Natural resin - translucent, off-white hemispheres. Flame and smoke suppressant. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mecha.. |
|||
Bulk Density | 0.961 g/cc | 0.0347 lb/in³ | |
Arkema Group KYNAR® 760 Polyvinylidene Fluoride Homopolymer - Extrusion Characteristics: Natural resin - translucent, off-white hemispheres. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechanical strength, low permeabili.. |
|||
Bulk Density | 0.961 g/cc | 0.0347 lb/in³ | |
Arkema Group KYNAR® 460 Polyvinylidene Fluoride Homopolymer - Extrusion Characteristics: Natural resin - translucent, off-white hemispheres. Broad molecular weight distribution. High stability in harsh thermal, chemical and ultraviolet environments. High toughness a.. |
|||
Bulk Density | 0.961 g/cc | 0.0347 lb/in³ | |
Arkema Group KYNAR® 460 Red Polyvinylidene Fluoride Homopolymer - Injection Molding and Extrusion Characteristics: Broad molecular weight distribution, pigmented. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechanical strength, low permeability, .. |
|||
Bulk Density | 0.961 g/cc | 0.0347 lb/in³ | |
Arkema Group KYNAR® 6000 HD Polyvinylidene Fluoride - Injection Molding Characteristics: Natural resin - translucent, off-white hemispheres. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechanical strength, low permeabili.. |
|||
Bulk Density | 0.961 g/cc | 0.0347 lb/in³ | |
Arkema Group KYNAR® EXAD 3000 Polyvinylidene Fluoride - Extrusion Characteristics: Natural resin - translucent, off-white hemispheres. Extrusion aid, lubricated. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechanic.. |
|||
Bulk Density | 0.960 g/cc | 0.0347 lb/in³ | |
Zircar Zirconia ZYZ-6 Zirconia Boards and Discs Insulation Type ZYZ Boards and Discs are rigid, refractory structures composed of yttria-stabilized zirconia fibers that are bonded with silica. This unique composition provides Type ZYZ insulation with the lo.. |
|||
Bulk Density | 0.961 g/cc | 0.0347 lb/in³ | |
Arkema Group KYNAR FLEX® 2800-20 Polyvinylidene Fluoride Copolymer - Extrusion & Molding Characteristics: Natural resin - translucent, off-white hemispheres. Flexible. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechanical strength, low.. |
|||
Bulk Density | 0.961 g/cc | 0.0347 lb/in³ | |
Arkema Group KYNAR FLEX® 2850-00 Polyvinylidene Fluoride Copolymer - Extrusion & Molding Characteristics: Natural resin - translucent, off-white hemispheres. 150°C Temperature rating. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechani.. |
|||
Bulk Density | 0.961 g/cc | 0.0347 lb/in³ | |
Arkema Group KYNAR FLEX® 2850-07 Polyvinylidene Fluoride Copolymer - Extrusion & Molding Characteristics: Natural resin - translucent, off-white hemispheres. 150°C Temperature rating. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechani.. |