Physical Properties | Metric | English | Comments |
---|---|---|---|
Bulk Density | 0.0300 g/cc | 0.00108 lb/in³ | Minimum |
SYNTHOS Koplen® 0513 FR Expandable Polystyrene Low Pentane Self-Extinguishing type Koplen®.Processing Method: Expansion of beads by water steam, hot water or hot air. Shaping into products and smaller blocks. Lower density can be achieved aft.. |
|||
Bulk Density | 0.0300 g/cc | 0.00108 lb/in³ | Scott |
TIMCAL TIMREX® BNB90 Expanded Graphite TIMREX Natural Flake Graphite is produced in a wide range of products distinguished by particle size distribution, chemistry and carbon content. Timcal mines the graphite from its own source in Lac-.. |
|||
Bulk Density | 0.0300 - 0.0360 g/cc | 0.00108 - 0.00130 lb/in³ | |
BASF Neopolen® P 9035 0.035 g/cc Core density; Expanded Polypropylene (Europe) Description: Neopolen® P 9035 is expanded Polypropylene supplied in the form of beads. The cells are largely closed.Physical properties of moldings made from Neopolen® P 9035.Note: In order to mea.. |
|||
Bulk Density | 0.0300 - 0.0360 g/cc | 0.00108 - 0.00130 lb/in³ | |
BASF Neopolen® P 9035 0.04 g/cc Core density; Expanded Polypropylene (Europe) Description: Neopolen® P 9035 is expanded Polypropylene supplied in the form of beads. The cells are largely closed.Physical properties of moldings made from Neopolen® P 9035.Note: In order to mea.. |
|||
Bulk Density | 0.0300 - 0.0360 g/cc | 0.00108 - 0.00130 lb/in³ | |
BASF Neopolen® P 9035 0.05 g/cc Core density; Expanded Polypropylene (Europe) Description: Neopolen® P 9035 is expanded Polypropylene supplied in the form of beads. The cells are largely closed.Physical properties of moldings made from Neopolen® P 9035.Note: In order to mea.. |
|||
Bulk Density | 0.0300 - 0.0360 g/cc | 0.00108 - 0.00130 lb/in³ | |
BASF Neopolen® P 9035 0.06 g/cc Core density; Expanded Polypropylene (Europe) Description: Neopolen® P 9035 is expanded Polypropylene supplied in the form of beads. The cells are largely closed.Physical properties of moldings made from Neopolen® P 9035.Note: In order to mea.. |
|||
Bulk Density | 0.0300 - 0.0360 g/cc | 0.00108 - 0.00130 lb/in³ | |
BASF Neopolen® P 9035 0.07 g/cc Core density; Expanded Polypropylene (Europe) Description: Neopolen® P 9035 is expanded Polypropylene supplied in the form of beads. The cells are largely closed.Physical properties of moldings made from Neopolen® P 9035.Note: In order to mea.. |
|||
Bulk Density | 0.0300 - 0.0360 g/cc | 0.00108 - 0.00130 lb/in³ | |
BASF Neopolen® P 9235 0.04 g/cc Core density; Expanded Polypropylene (Europe) Description: Neopolen® P 9235 is expanded Polypropylene supplied in the form of beads. The cells are largely closed.Physical properties of moldings made from Neopolen® P 9235.Note: In order to mea.. |
|||
Bulk Density | 0.0300 - 0.0360 g/cc | 0.00108 - 0.00130 lb/in³ | |
BASF Neopolen® P 9435 0.04 g/cc Core density; Expanded Polypropylene (Europe) Description: Neopolen® P 9435 is expanded Polypropylene supplied in the form of beads. The cells are largely closed.Physical properties of moldings made from Neopolen® P 9435.Note: In order to mea.. |
|||
Bulk Density | 0.0300 - 0.0360 g/cc | 0.00108 - 0.00130 lb/in³ | |
BASF Neopolen® P 9435 0.05 g/cc Core density; Expanded Polypropylene (Europe) Description: Neopolen® P 9435 is expanded Polypropylene supplied in the form of beads. The cells are largely closed.Physical properties of moldings made from Neopolen® P 9435.Note: In order to mea.. |
|||
Bulk Density | 0.0300 - 0.0360 g/cc | 0.00108 - 0.00130 lb/in³ | |
BASF Neopolen® P 9435 0.06 g/cc Core density; Expanded Polypropylene (Europe) Description: Neopolen® P 9435 is expanded Polypropylene supplied in the form of beads. The cells are largely closed.Physical properties of moldings made from Neopolen® P 9435.Note: In order to mea.. |
|||
Bulk Density | 0.0300 - 0.0360 g/cc | 0.00108 - 0.00130 lb/in³ | |
BASF Neopolen® P 9235 0.035 g/cc Core density; Expanded Polypropylene (Europe) Description: Neopolen® P 9235 is expanded Polypropylene supplied in the form of beads. The cells are largely closed.Physical properties of moldings made from Neopolen® P 9235.Note: In order to mea.. |
|||
Bulk Density | 0.0300 - 0.0360 g/cc | 0.00108 - 0.00130 lb/in³ | |
BASF Neopolen® P 9235 0.05 g/cc Core density; Expanded Polypropylene (Europe) Description: Neopolen® P 9235 is expanded Polypropylene supplied in the form of beads. The cells are largely closed.Physical properties of moldings made from Neopolen® P 9235.Note: In order to mea.. |
|||
Bulk Density | 0.0300 - 0.0360 g/cc | 0.00108 - 0.00130 lb/in³ | |
BASF Neopolen® P 9235 0.06 g/cc Core density; Expanded Polypropylene (Europe) Description: Neopolen® P 9235 is expanded Polypropylene supplied in the form of beads. The cells are largely closed.Physical properties of moldings made from Neopolen® P 9235.Note: In order to mea.. |
|||
Bulk Density | 0.0300 - 0.0360 g/cc | 0.00108 - 0.00130 lb/in³ | |
BASF Neopolen® P 9235 0.07 g/cc Core density; Expanded Polypropylene (Europe) Description: Neopolen® P 9235 is expanded Polypropylene supplied in the form of beads. The cells are largely closed.Physical properties of moldings made from Neopolen® P 9235.Note: In order to mea.. |
|||
Bulk Density | 0.0300 - 0.0360 g/cc | 0.00108 - 0.00130 lb/in³ | |
BASF Neopolen® P 9435 0.07 g/cc Core density; Expanded Polypropylene (Europe) Description: Neopolen® P 9435 is expanded Polypropylene supplied in the form of beads. The cells are largely closed.Physical properties of moldings made from Neopolen® P 9435.Note: In order to mea.. |
|||
Bulk Density | 0.0300 - 0.0360 g/cc | 0.00108 - 0.00130 lb/in³ | |
BASF Neopolen® P 9435 0.035 g/cc Core density; Expanded Polypropylene (Europe) Description: Neopolen® P 9435 is expanded Polypropylene supplied in the form of beads. The cells are largely closed.Physical properties of moldings made from Neopolen® P 9435.Note: In order to mea.. |