Physical Properties | Metric | English | Comments |
---|---|---|---|
Bulk Density | 0.0200 - 0.0400 g/cc | 0.000723 - 0.00145 lb/in³ | Typical |
SYNTHOS Koplen® 2040 F Expandable Polystyrene Self-Extinguishing type Koplen®.Processing Method: Pre-expansion of beads by water steam, hot water or hot air. Shaping into blocks.Specific Characteristics: Flammability according to CSN EN ISO .. |
|||
Bulk Density | 0.0200 g/cc | 0.000723 lb/in³ | After expansion; ASTM D3575 |
Sekisui PIOCELAN LP-50E Moldable Polymer Foam A hybrid moldable resin material PIOCLEAN, consisting of polystyrene and polyolefin, achieves performance exceeding that of the individual components by effectively combining materials with drastica.. |
|||
Bulk Density | 0.0200 g/cc | 0.000723 lb/in³ | After expansion; ASTM D3575 |
Sekisui PIOCELAN LSP-50EB Moldable Polymer Foam A hybrid moldable resin material PIOCLEAN, consisting of polystyrene and polyolefin, achieves performance exceeding that of the individual components by effectively combining materials with drastica.. |
|||
Bulk Density | 0.0200 g/cc | 0.000723 lb/in³ | After expansion; ASTM D3575 |
Sekisui PIOCELAN SP-50D Moldable Polymer Foam A hybrid moldable resin material PIOCLEAN, consisting of polystyrene and polyolefin, achieves performance exceeding that of the individual components by effectively combining materials with drastica.. |
|||
Bulk Density | 0.0200 g/cc | 0.000723 lb/in³ | After expansion; ASTM D3575 |
Sekisui PIOCELAN SP-50E Moldable Polymer Foam A hybrid moldable resin material PIOCLEAN, consisting of polystyrene and polyolefin, achieves performance exceeding that of the individual components by effectively combining materials with drastica.. |