Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Bulk Density = 0.0141 lb/in³ Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Bulk Density 0.330 - 0.390 g/cc
0.0119 - 0.0141 lb/in³
ASTM D1895
Polimeros Mexicanos Rotofoam® Plus 93050 Medium Density Polyethylene, Foam Grade
Hexene Copolymer Linear Medium Density Polyethylene for foaming applications. It is formulated for inner layers with excellent foam cell structure and smooth surface finish and uniform closed cells...
Bulk Density 0.330 - 0.390 g/cc
0.0119 - 0.0141 lb/in³
ASTM D1895
Polimeros Mexicanos Rotolene® 93050 Medium Density Polyethylene
Hexene Copolymer Linear Medium Density Polyethylene for rotational molding. This resin is fully UV8 stabilized.Recommended for general purpose applications. Frequently used for water tanks (less tha..
Bulk Density 0.330 - 0.390 g/cc
0.0119 - 0.0141 lb/in³
ASTM D1895
Polimeros Mexicanos Rotolene® 93835-TG Medium Density Polyethylene
MDPE Copolymer with UV8 stabilizer in natural and colors.Recommended for rotomolding. Used for manufacture of water tanks > 2000 liters, cisterns, farm tanks, or tanks to contain strong acids and b..
Bulk Density 0.330 - 0.390 g/cc
0.0119 - 0.0141 lb/in³
ASTM D1895
Polimeros Mexicanos Rotolene® Black Plus Polyethylene
Polyethylene compound specially formulated for rotational molding applications requiring good mechanical properties and good mold release properties. Rotational molded parts have smooth surface and ..
Bulk Density 0.330 - 0.390 g/cc
0.0119 - 0.0141 lb/in³
ASTM D1895-96
Polimeros Mexicanos Rotolene® Black Plus Ultra Polyethylene
Linear copolymer Medium Density Polyethylene which is fully UV8 stabilized. Available as black powder.Applications: Polyethylene compound specially formulated for rotational molding applications req..
Bulk Density 0.330 - 0.390 g/cc
0.0119 - 0.0141 lb/in³
ASTM D1895
Polimeros Mexicanos Rotolene® Diesel Tank Medium Density Polyethylene
Hexene Copolymer Linear Medium Density Polyethylene. This resin is fully UV8 stabilized.High quality Polyethylene compound specially designed for automotive applications, water tanks, diesel tanks a..
Bulk Density 0.290 - 0.390 g/cc
0.0105 - 0.0141 lb/in³
ASTM D1895
LG Chemical LK170 PVC
General Description: LK170, vinyl chloride copolymer with vinyl acetate exhibit excellent properties including easy processing and effective flowMain Applications: Sealant, automotive protective sol..
Bulk Density 0.290 - 0.390 g/cc
0.0105 - 0.0141 lb/in³
ASTM D1895
LG Chemical LP090 PVC
General Description: LP090 ,Homopolymer made from micro-suspension polymerization ,is a medium-viscosity PVC resin with a pseudo plastic flow property in processing range. LP090 can be used for wall..
Bulk Density 0.290 - 0.390 g/cc
0.0105 - 0.0141 lb/in³
ASTM D1895
LG Chemical LP170G PVC
General Description: LP170G, homopolymer made from micro- suspension polymerization, is a low viscosity PVC resin with an good deaeration and stable viscosity at high temperature. Products made from..
Bulk Density 0.290 - 0.390 g/cc
0.0105 - 0.0141 lb/in³
ASTM D1895
LG Chemical LP170L PVC
General Description: LP170L, homopolymer made from micro- suspension polymerization, is a medium- viscosity PVC resin with a pseudo plastic flow property in processing range. LP170L can be used for ..
Bulk Density 0.0190 - 0.390 g/cc
0.000686 - 0.0141 lb/in³
Dependent on grade.
Destech Open-Celled Glassy Carbon Foam
Destech glassy (vitreous) carbon foam is available in different grades depending on the number of pores per inch (ppi). Standard grades are 10, 45, 100 and 500 ppi. Custom grades are available on a..
Copyright © lookpolymers.com All Rights Reserved