Polymer Property : Linear Mold Shrinkage, Transverse = 0.018 cm/cm Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Linear Mold Shrinkage, Transverse 0.016 - 0.018 cm/cm

@Time 86400 sec
0.016 - 0.018 in/in

@Time 24.0 hour
ASTM D955
SABIC Innovative Plastics LNP LUBRICOMP RFL33 PA 66
LNP* LUBRICOMP* RFL33 is a compound based on Nylon 66 resin containing 15% Glass Fiber, 15% PTFE. Added feature of this material is: Wear Resistant.
Linear Mold Shrinkage, Transverse 0.016 - 0.018 cm/cm

@Time 86400 sec
0.016 - 0.018 in/in

@Time 24.0 hour
ASTM D955
SABIC Innovative Plastics LNP LUBRICOMP RFL33 PA 66 (Asia Pacific)
LNP* Lubricomp* RFL33 is a compound based on Nylon 66 resin containing Glass Fiber, PTFE. Added features of this material include: Internally Lubricated.
Linear Mold Shrinkage, Transverse 0.016 - 0.018 cm/cm

@Time 86400 sec
0.016 - 0.018 in/in

@Time 24.0 hour
ASTM D955
SABIC Innovative Plastics LNP LUBRILOY U2000A PPA
LNP* LUBRILOY* U2000A is a compound based on Polyphthalamide resin containing Proprietary Lubricant. Added feature of this material is: Wear Resistant.
Linear Mold Shrinkage, Transverse 0.016 - 0.018 cm/cm

@Time 86400 sec
0.016 - 0.018 in/in

@Time 24.0 hour
ASTM D955
SABIC Innovative Plastics LNP LUBRILOY U2000A PPA (Asia Pacific)
LNP* Lubriloy* U2000A is a compound based on Polyphthalamide resin containing Proprietary Lubricant. Added features of this material include: Internally Lubricated.
Linear Mold Shrinkage, Transverse 0.016 - 0.018 cm/cm

@Time 86400 sec
0.016 - 0.018 in/in

@Time 24.0 hour
ASTM D955
SABIC Innovative Plastics LNP STAT-KON KE004 Acetal Copoly
LNP* STAT-KON* KE004 is a compound based on Acetal Copolymer resin containing 20% Carbon Fiber. Added features of this material include: Electrically Conductive.
Linear Mold Shrinkage, Transverse 0.016 - 0.018 cm/cm

@Time 86400 sec
0.016 - 0.018 in/in

@Time 24.0 hour
ASTM D955
SABIC Innovative Plastics LNP STAT-KON KE004 Acetal Copoly (Asia Pacific)
LNP* Stat-kon* KE004 is a compound based on Acetal Copolymer resin containing Carbon Fiber. Added features of this material include: Electrically Conductive.
Linear Mold Shrinkage, Transverse 0.0158 - 0.018 cm/cm

@Time 86400 sec
0.0158 - 0.018 in/in

@Time 24.0 hour
ISO 294
SABIC Innovative Plastics LNP STAT-KON MD000IS PP
LNP STAT-KON* MD000IS is a compound based on Polypropylene resin containing Carbon Powder. Added features of this material include: Electrically Conductive, High Impact.
Linear Mold Shrinkage, Transverse 0.016 - 0.018 cm/cm

@Time 86400 sec
0.016 - 0.018 in/in

@Time 24.0 hour
ASTM D955
SABIC Innovative Plastics LNP STAT-KON MD000IS PP
LNP STAT-KON* MD000IS is a compound based on Polypropylene resin containing Carbon Powder. Added features of this material include: Electrically Conductive, High Impact.
Linear Mold Shrinkage, Transverse 0.0158 - 0.018 cm/cm

@Time 86400 sec
0.0158 - 0.018 in/in

@Time 24.0 hour
ISO 294
SABIC Innovative Plastics LNP STAT-KON MD000ISC PP (Asia Pacific)
LNP STAT-KON* MD000ISC is a compound based on Polypropylene resin containing Carbon Powder. Added features of this material include: Electrically Conductive.
Linear Mold Shrinkage, Transverse 0.016 - 0.018 cm/cm

@Time 86400 sec
0.016 - 0.018 in/in

@Time 24.0 hour
ASTM D955
SABIC Innovative Plastics LNP STAT-KON MD000ISC PP (Asia Pacific)
LNP STAT-KON* MD000ISC is a compound based on Polypropylene resin containing Carbon Powder. Added features of this material include: Electrically Conductive.
Linear Mold Shrinkage, Transverse 0.0158 - 0.018 cm/cm

@Time 86400 sec
0.0158 - 0.018 in/in

@Time 24.0 hour
ISO 294
SABIC Innovative Plastics LNP STAT-KON MD000ISC PP
LNP STAT-KON* MD000ISC is a compound based on Polypropylene resin containing Carbon Powder. Added features of this material include: Electrically Conductive, High Impact.
Linear Mold Shrinkage, Transverse 0.016 - 0.018 cm/cm

@Time 86400 sec
0.016 - 0.018 in/in

@Time 24.0 hour
ASTM D955
SABIC Innovative Plastics LNP STAT-KON MD000ISC PP
LNP STAT-KON* MD000ISC is a compound based on Polypropylene resin containing Carbon Powder. Added features of this material include: Electrically Conductive, High Impact.
Linear Mold Shrinkage, Transverse 0.016 - 0.018 cm/cm

@Time 86400 sec
0.016 - 0.018 in/in

@Time 24.0 hour
ASTM D 955
SABIC Innovative Plastics LNP Stat-kon MD000IU PP
LNP* Stat-kon* MD000IU is a compound based on Polypropylene resin containing Carbon Powder. Added features of this material include: Electrically Conductive, High Impact, UV Stabilized.This data wa..
Linear Mold Shrinkage, Transverse 0.016 - 0.018 cm/cm

@Time 86400 sec
0.016 - 0.018 in/in

@Time 24.0 hour
ISO 294
SABIC Innovative Plastics LNP Stat-kon MD000IU PP
LNP* Stat-kon* MD000IU is a compound based on Polypropylene resin containing Carbon Powder. Added features of this material include: Electrically Conductive, High Impact, UV Stabilized.This data wa..
Linear Mold Shrinkage, Transverse 0.016 - 0.018 cm/cm

@Time 86400 sec
0.016 - 0.018 in/in

@Time 24.0 hour
ASTM D 955
SABIC Innovative Plastics LNP Stat-kon MD000IU PP (Asia Pacific)
LNP* Stat-kon* MD000IU is a compound based on Polypropylene resin containing Carbon Powder. Added features of this material include: Electrically Conductive, High Impact, UV Stabilized.This data wa..
Linear Mold Shrinkage, Transverse 0.016 - 0.018 cm/cm

@Time 86400 sec
0.016 - 0.018 in/in

@Time 24.0 hour
ISO 294
SABIC Innovative Plastics LNP Stat-kon MD000IU PP (Asia Pacific)
LNP* Stat-kon* MD000IU is a compound based on Polypropylene resin containing Carbon Powder. Added features of this material include: Electrically Conductive, High Impact, UV Stabilized.This data wa..