Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage, Transverse | 0.016 cm/cm @Time 86400 sec |
0.016 in/in @Time 24.0 hour |
ASTM D955 |
SABIC Innovative Plastics LNP LUBRICOMP KZL16 Acetal Copolymer LNP LUBRICOMP* KZL16 is a compound based on Acetal Copolymer resin containing Glass Fiber, Milled Glass, PTFE. Added features of this material include: Internally Lubricated. |
|||
Linear Mold Shrinkage, Transverse | 0.016 - 0.018 cm/cm @Time 86400 sec |
0.016 - 0.018 in/in @Time 24.0 hour |
ASTM D955 |
SABIC Innovative Plastics LNP LUBRICOMP RFL33 PA 66 LNP* LUBRICOMP* RFL33 is a compound based on Nylon 66 resin containing 15% Glass Fiber, 15% PTFE. Added feature of this material is: Wear Resistant. |
|||
Linear Mold Shrinkage, Transverse | 0.016 - 0.018 cm/cm @Time 86400 sec |
0.016 - 0.018 in/in @Time 24.0 hour |
ASTM D955 |
SABIC Innovative Plastics LNP LUBRICOMP RFL33 PA 66 (Asia Pacific) LNP* Lubricomp* RFL33 is a compound based on Nylon 66 resin containing Glass Fiber, PTFE. Added features of this material include: Internally Lubricated. |
|||
Linear Mold Shrinkage, Transverse | 0.016 - 0.018 cm/cm @Time 86400 sec |
0.016 - 0.018 in/in @Time 24.0 hour |
ASTM D955 |
SABIC Innovative Plastics LNP LUBRILOY U2000A PPA LNP* LUBRILOY* U2000A is a compound based on Polyphthalamide resin containing Proprietary Lubricant. Added feature of this material is: Wear Resistant. |
|||
Linear Mold Shrinkage, Transverse | 0.016 - 0.018 cm/cm @Time 86400 sec |
0.016 - 0.018 in/in @Time 24.0 hour |
ASTM D955 |
SABIC Innovative Plastics LNP LUBRILOY U2000A PPA (Asia Pacific) LNP* Lubriloy* U2000A is a compound based on Polyphthalamide resin containing Proprietary Lubricant. Added features of this material include: Internally Lubricated. |
|||
Linear Mold Shrinkage, Transverse | 0.016 - 0.024 cm/cm @Thickness 2.30 - 4.60 mm |
0.016 - 0.024 in/in @Thickness 0.0906 - 0.181 in |
SABIC Method |
SABIC Innovative Plastics Valox® 195HP PBT PELLET FORM. For compounding only (not for injection molding). Unreinforced PBT. FDA 21CFR177.1660 compliant. Melt viscosity between 740 and 900 poise. Natural Color (1001) Only. |
|||
Linear Mold Shrinkage, Transverse | 0.016 - 0.024 cm/cm @Thickness 2.30 - 4.60 mm |
0.016 - 0.024 in/in @Thickness 0.0906 - 0.181 in |
SABIC Method |
SABIC Innovative Plastics Valox® 215HPR PBT Unreinforced PBT with mold release. FDA food contact compliant in limited colors. Effective March 2008 this grade will no longer be supported with biocompatibility data. Alternative grade Valox HX21.. |
|||
Linear Mold Shrinkage, Transverse | 0.016 - 0.024 cm/cm @Thickness 2.30 - 4.60 mm |
0.016 - 0.024 in/in @Thickness 0.0906 - 0.181 in |
SABIC Method |
SABIC Innovative Plastics Valox® 295 PBT Unreinforced PBTThis data was supplied by SABIC-IP for the Americas region. |
|||
Linear Mold Shrinkage, Transverse | 0.016 - 0.024 cm/cm @Thickness 2.30 - 4.60 mm |
0.016 - 0.024 in/in @Thickness 0.0906 - 0.181 in |
SABIC Method |
SABIC Innovative Plastics Valox® 310 PBT Unreinforced, general purpose. Typical viscosity 5000-7000. |
|||
Linear Mold Shrinkage, Transverse | 0.016 - 0.024 cm/cm @Thickness 2.30 - 4.60 mm |
0.016 - 0.024 in/in @Thickness 0.0906 - 0.181 in |
SABIC Method |
SABIC Innovative Plastics Valox® 311 PBT Unreinforced, improved resistance to UV. Medium viscosity. |
|||
Linear Mold Shrinkage, Transverse | 0.016 - 0.024 cm/cm @Thickness 2.30 - 4.60 mm |
0.016 - 0.024 in/in @Thickness 0.0906 - 0.181 in |
SABIC Method |
SABIC Innovative Plastics Valox® 312 PBT (Asia Pacific) Unreinforced, For compounding only (not for injection molding), Medium viscosity. |
|||
Linear Mold Shrinkage, Transverse | 0.016 - 0.024 cm/cm @Thickness 2.30 - 4.60 mm |
0.016 - 0.024 in/in @Thickness 0.0906 - 0.181 in |
SABIC Method |
SABIC Innovative Plastics Valox® 315 PBT Unreinforced, For extrusion/compounding only (not for injection molding). High viscosity. Melt viscosity between 7500 and 9500 poise. |
|||
Linear Mold Shrinkage, Transverse | 0.016 - 0.024 cm/cm @Thickness 2.30 - 4.60 mm |
0.016 - 0.024 in/in @Thickness 0.0906 - 0.181 in |
SABIC Method |
SABIC Innovative Plastics Valox® 325 PBT (Asia Pacific) General purpose, unreinforced, improved processing. Applications like sprinklers and nozzles, pumps, door handle, tank covers, pens, pencils etc. |
|||
Linear Mold Shrinkage, Transverse | 0.016 - 0.024 cm/cm @Thickness 2.30 - 4.60 mm |
0.016 - 0.024 in/in @Thickness 0.0906 - 0.181 in |
SABIC Method |
SABIC Innovative Plastics Valox® 325M PBT (Asia Pacific) 325M is a high flow VALOX 325 for restrictive gate tooling (key buttons)This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Linear Mold Shrinkage, Transverse | 0.016 - 0.018 cm/cm @Time 86400 sec |
0.016 - 0.018 in/in @Time 24.0 hour |
ASTM D955 |
SABIC Innovative Plastics LNP STAT-KON KE004 Acetal Copoly LNP* STAT-KON* KE004 is a compound based on Acetal Copolymer resin containing 20% Carbon Fiber. Added features of this material include: Electrically Conductive. |
|||
Linear Mold Shrinkage, Transverse | 0.016 - 0.018 cm/cm @Time 86400 sec |
0.016 - 0.018 in/in @Time 24.0 hour |
ASTM D955 |
SABIC Innovative Plastics LNP STAT-KON KE004 Acetal Copoly (Asia Pacific) LNP* Stat-kon* KE004 is a compound based on Acetal Copolymer resin containing Carbon Fiber. Added features of this material include: Electrically Conductive. |
|||
Linear Mold Shrinkage, Transverse | 0.016 - 0.018 cm/cm @Time 86400 sec |
0.016 - 0.018 in/in @Time 24.0 hour |
ASTM D955 |
SABIC Innovative Plastics LNP STAT-KON MD000IS PP LNP STAT-KON* MD000IS is a compound based on Polypropylene resin containing Carbon Powder. Added features of this material include: Electrically Conductive, High Impact. |
|||
Linear Mold Shrinkage, Transverse | 0.016 - 0.018 cm/cm @Time 86400 sec |
0.016 - 0.018 in/in @Time 24.0 hour |
ASTM D955 |
SABIC Innovative Plastics LNP STAT-KON MD000ISC PP (Asia Pacific) LNP STAT-KON* MD000ISC is a compound based on Polypropylene resin containing Carbon Powder. Added features of this material include: Electrically Conductive. |
|||
Linear Mold Shrinkage, Transverse | 0.016 cm/cm @Time 86400 sec |
0.016 in/in @Time 24.0 hour |
ISO 294 |
SABIC Innovative Plastics LNP THERMOCOMP KF002L Acetal Homopoly (Asia Pacific) LNP* Thermocomp* KF002L is a compound based on Acetal Homopolymer resin containing Glass Fiber. Added features of this material include: Low Extractible. |
|||
Linear Mold Shrinkage, Transverse | 0.016 cm/cm @Time 86400 sec |
0.016 in/in @Time 24.0 hour |
ASTM D955 |
SABIC Innovative Plastics LNP THERMOCOMP KF006XXC Acetal Copolymer (Asia Pacific) LNP* Thermocomp* KF006XXC is a compound based on Acetal Copolymer resin containing Glass Fiber. |
|||
Linear Mold Shrinkage, Transverse | 0.016 cm/cm @Time 86400 sec |
0.016 in/in @Time 24.0 hour |
ISO 294 |
SABIC Innovative Plastics LNP THERMOCOMP KF006XXC Acetal Copolymer (Asia Pacific) LNP* Thermocomp* KF006XXC is a compound based on Acetal Copolymer resin containing Glass Fiber. |
|||
Linear Mold Shrinkage, Transverse | 0.016 cm/cm @Time 86400 sec |
0.016 in/in @Time 24.0 hour |
ASTM D 955 |
SABIC Innovative Plastics LNP Thermocomp WFB51 PBT LNP THERMOCOMP* WFB51 is a compound based on Polybutylene Terephalate resin containing Glass Bead, Glass Fiber. Added features of this material include: Low Warpage.This data was supplied by SABIC-.. |
|||
Linear Mold Shrinkage, Transverse | 0.016 cm/cm @Time 86400 sec |
0.016 in/in @Time 24.0 hour |
ISO 294 |
SABIC Innovative Plastics LNP THERMOCOMP WFB54 PBT LNP* THERMOCOMP* WFB54 is a compound based on PBT resin containing 20% Glass Fiber, 25% Glass Bead. |
|||
Linear Mold Shrinkage, Transverse | 0.016 cm/cm @Temperature 240 °C |
0.016 in/in @Temperature 464 °F |
ASTM D3392 |
DuPont™ Nomex® Type 993, 60 mil Nominal Thickness Medium-Density Aromatic Nylon Pressboard Type 993 is a medium-density pressboard which offers a balance of rigidity and conformability along with outstanding saturability and excellent properties in air and oil. Typical applications includ.. |
|||
Linear Mold Shrinkage, Transverse | 0.016 cm/cm @Thickness 3.17 mm |
0.016 in/in @Thickness 0.125 in |
|
Advanced Polymer Alloys DuraGrip™ DGR 6030 NC/BK Thermoplastic Elastomer (TPE) DuraGrip® DGR 6030 NC/BK are designed to be general purpose Thermoplastic Elastomers (TPE) that are easy to use in injection molding and extrusion processes. DGR 6030 NC/BK have
an excellent soft t.. |
|||
Linear Mold Shrinkage, Transverse | 0.016 - 0.018 cm/cm @Time 86400 sec |
0.016 - 0.018 in/in @Time 24.0 hour |
ASTM D955 |
SABIC Innovative Plastics LNP STAT-KON MD000ISC PP LNP STAT-KON* MD000ISC is a compound based on Polypropylene resin containing Carbon Powder. Added features of this material include: Electrically Conductive, High Impact. |
|||
Linear Mold Shrinkage, Transverse | 0.016 - 0.018 cm/cm @Time 86400 sec |
0.016 - 0.018 in/in @Time 24.0 hour |
ASTM D 955 |
SABIC Innovative Plastics LNP Stat-kon MD000IU PP LNP* Stat-kon* MD000IU is a compound based on Polypropylene resin containing Carbon Powder. Added features of this material include: Electrically Conductive, High Impact, UV Stabilized.This data wa.. |
|||
Linear Mold Shrinkage, Transverse | 0.016 - 0.018 cm/cm @Time 86400 sec |
0.016 - 0.018 in/in @Time 24.0 hour |
ISO 294 |
SABIC Innovative Plastics LNP Stat-kon MD000IU PP LNP* Stat-kon* MD000IU is a compound based on Polypropylene resin containing Carbon Powder. Added features of this material include: Electrically Conductive, High Impact, UV Stabilized.This data wa.. |
|||
Linear Mold Shrinkage, Transverse | 0.016 - 0.018 cm/cm @Time 86400 sec |
0.016 - 0.018 in/in @Time 24.0 hour |
ASTM D 955 |
SABIC Innovative Plastics LNP Stat-kon MD000IU PP (Asia Pacific) LNP* Stat-kon* MD000IU is a compound based on Polypropylene resin containing Carbon Powder. Added features of this material include: Electrically Conductive, High Impact, UV Stabilized.This data wa.. |
|||
Linear Mold Shrinkage, Transverse | 0.016 - 0.018 cm/cm @Time 86400 sec |
0.016 - 0.018 in/in @Time 24.0 hour |
ISO 294 |
SABIC Innovative Plastics LNP Stat-kon MD000IU PP (Asia Pacific) LNP* Stat-kon* MD000IU is a compound based on Polypropylene resin containing Carbon Powder. Added features of this material include: Electrically Conductive, High Impact, UV Stabilized.This data wa.. |