Polymer Property : Linear Mold Shrinkage, Transverse = 0.0087 in/in Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Linear Mold Shrinkage, Transverse 0.0087 cm/cm

@Time 86400 sec
0.0087 in/in

@Time 24.0 hour
ISO 294
SABIC Innovative Plastics LNP LUBRICOMP ZL003 PPE+PS
LNP* LUBRICOMP* ZL003 is a compound based on PPE+PS resin containing 15% PTFE. Added features of this material include: Wear Resistant.
Linear Mold Shrinkage, Transverse 0.0087 cm/cm

@Time 86400 sec
0.0087 in/in

@Time 24.0 hour
ISO 294
SABIC Innovative Plastics LNP LUBRICOMP ZL003 PPE+PS (Asia Pacific)
LNP LUBRICOMP ZL003 is a compound based on PPE+PS Blend resin containing PTFE. Added features of this material include:internally Lubricated. Also known as LUBRICOMP ZL-4030