Polymer Property : Linear Mold Shrinkage, Transverse = 0.0058 in/in Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Linear Mold Shrinkage, Transverse 0.0058 cm/cm

@Time 86400 sec
0.0058 in/in

@Time 24.0 hour
ISO 294
SABIC Innovative Plastics LNP THERMOCOMP GF006 PSU
LNP THERMOCOMP* GF006 is a compound based on Polysulfone resin containing 30% Glass Fiber.
Linear Mold Shrinkage, Transverse 0.0058 cm/cm

@Time 86400 sec
0.0058 in/in

@Time 24.0 hour
ISO 294
SABIC Innovative Plastics LNP THERMOCOMP GF006XXZ PSU
LNP THERMOCOMP* GF006XXZ is a compound based on Polysulfone resin containing 30% Glass Fiber.
Linear Mold Shrinkage, Transverse 0.0058 cm/cm

@Time 86400 sec
0.0058 in/in

@Time 24.0 hour
ISO 294
SABIC Innovative Plastics LNP THERMOCOMP LF004E PEEK (Asia Pacific)
LNP* Thermocomp* LF004E is a compound based on Polyetheretherketone resin containing Glass Fiber. Added features of this material include: Easy Molding.
Linear Mold Shrinkage, Transverse 0.0058 cm/cm

@Time 86400 sec
0.0058 in/in

@Time 24.0 hour
ISO 294
SABIC Innovative Plastics LNP THERMOCOMP NF004 PC+ABS
LNP* THERMOCOMP* NF004 is a compound based on PC+ABS resin containing 20% Glass Fiber.
Linear Mold Shrinkage, Transverse 0.0058 cm/cm

@Time 86400 sec
0.0058 in/in

@Time 24.0 hour
ISO 294
SABIC Innovative Plastics LNP THERMOCOMP NF004 PC+ABS (Asia Pacific)
LNP* Thermocomp* NF004 is a compound based on PC+ABS Blend resin containing Glass Fiber.