Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage, Transverse | 0.0053 cm/cm @Thickness 2.00 mm |
0.0053 in/in @Thickness 0.0787 in |
2x60x60mm; ASTM D955 |
Lavergne VYPET VNT 340 PET 40% Glass - Mineral Reinforced Vypet VNT 340 is a 40% glass/mineral reinforced PET injection molding compound designed for electrical and structural applications, with High Dielectric StrengthFeatures: High temperature performanc.. |
|||
Linear Mold Shrinkage, Transverse | 0.0053 cm/cm @Time 86400 sec |
0.0053 in/in @Time 24.0 hour |
ISO 294 |
SABIC Innovative Plastics LNP LUBRICOMP OX88533 PPS LNP LUBRICOMP* OX88533 is a compound based on Polyphenylene Sulfide resin containing Proprietary Filler(s). Added feature of this material is: Wear Resistant. |
|||
Linear Mold Shrinkage, Transverse | 0.0053 cm/cm @Time 86400 sec |
0.0053 in/in @Time 24.0 hour |
ISO 294 |
SABIC Innovative Plastics LNP STAT-KON ZE004 MODIFIED POLYPHENYLENE (Asia Pacific) LNP* Stat-kon* ZE004 is a compound based on MODIFIED POYPHENYLENE resin containing Carbon Fiber. |
|||
Linear Mold Shrinkage, Transverse | 0.0053 cm/cm @Time 86400 sec |
0.0053 in/in @Time 24.0 hour |
ISO 294 |
SABIC Innovative Plastics LNP Stat-kon ZE004 MODIFIED POYPHENYLENE LNP* Stat-kon* ZE004 is a compound based on MODIFIED POYPHENYLENE resin containing Carbon Fiber.This data was supplied by SABIC-IP for the Americas region. |
|||
Linear Mold Shrinkage, Transverse | 0.0053 cm/cm @Time 86400 sec |
0.0053 in/in @Time 24.0 hour |
ISO 294 |
SABIC Innovative Plastics LNP Stat-kon ZE004 MODIFIED POYPHENYLENE (Asia Pacific) LNP* Stat-kon* ZE004 is a compound based on MODIFIED POYPHENYLENE resin containing Carbon Fiber.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Linear Mold Shrinkage, Transverse | 0.0053 cm/cm @Time 86400 sec |
0.0053 in/in @Time 24.0 hour |
ISO 294 |
SABIC Innovative Plastics LNP STAT-KON ZE004 PPO LNP* STAT-KON* ZE004 is a compound based on PPO resin containing 20% Carbon Fiber. Added feature of this grade includes: Electrically Conductive. |
|||
Linear Mold Shrinkage, Transverse | 0.0053 cm/cm @Time 86400 sec |
0.0053 in/in @Time 24.0 hour |
ISO 294 |
SABIC Innovative Plastics LNP VERTON MX02795 PP (Asia Pacific) LNP* Verton* MX02795 is a compound based on Polypropylene resin containing Long Glass Fiber. Added features of this material include: Chemically Coupled, Heat Stabilized, UV Stabilized. |
|||
Linear Mold Shrinkage, Transverse | 0.0053 cm/cm @Time 86400 sec |
0.0053 in/in @Time 24.0 hour |
ISO 294 |
SABIC Innovative Plastics LNP VERTON MX02795 PP LNP* VERTON* MX02795 is a compound based on Polypropylene resin containing Proprietary Fillers. Added features of this material include: Heat Stabilized, UV Stabilized, Structural. |