Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage, Transverse | 0.0050 - 0.0070 cm/cm @Time 86400 sec |
0.0050 - 0.0070 in/in @Time 24.0 hour |
ASTM D955 |
SABIC Innovative Plastics LNP LUBRICOMP DFL23 PC LNP* Lubricomp* DFL23 is a compound based on Polycarbonate resin containing 15% Glass Fiber and 10% PTFE. Added features include: Internally Lubricated. |
|||
Linear Mold Shrinkage, Transverse | 0.0050 - 0.010 cm/cm @Time 86400 sec |
0.0050 - 0.010 in/in @Time 24.0 hour |
ASTM D955 |
SABIC Innovative Plastics LNP LUBRICOMP WFL36 PBT LNP LUBRICOMP* WFL36 is a compound based on PBT resin containing 30% Glass Fiber, 15% PTFE. Added features of this material include: Wear Resistant. |
|||
Linear Mold Shrinkage, Transverse | 0.0050 - 0.010 cm/cm @Time 86400 sec |
0.0050 - 0.010 in/in @Time 24.0 hour |
ISO 294 |
SABIC Innovative Plastics LNP LUBRICOMP WFL36 PBT LNP LUBRICOMP* WFL36 is a compound based on PBT resin containing 30% Glass Fiber, 15% PTFE. Added features of this material include: Wear Resistant. |
|||
Linear Mold Shrinkage, Transverse | 0.0050 - 0.010 cm/cm @Time 86400 sec |
0.0050 - 0.010 in/in @Time 24.0 hour |
ISO 294 |
SABIC Innovative Plastics LNP LUBRICOMP WFP36 PBT LNP LUBRICOMP* WFP36 is a compound based on PBT resin containing 30% Glass Fiber, 15% PTFE/Silicone. Added features of this material include: Wear Resistant. |
|||
Linear Mold Shrinkage, Transverse | 0.0050 - 0.010 cm/cm @Time 86400 sec |
0.0050 - 0.010 in/in @Time 24.0 hour |
ISO 294 |
SABIC Innovative Plastics LNP LUBRICOMP WFP36 PBT (Asia Pacific) LNP LUBRICOMP* WFP36 is a compound based on Polybutylene Terephalate resin containing Silicone, Glass Fiber, PTFE. Added features of this material include: Internally Lubricated. |
|||
Linear Mold Shrinkage, Transverse | 0.0050 cm/cm @Time 86400 sec |
0.0050 in/in @Time 24.0 hour |
ASTM D955 |
SABIC Innovative Plastics LNP STAT-KON DEP42E PC LNP STAT-KON* DEP42E is a compound based on Polycarbonate resin containing 10% Carbon Fiber, 20% PTFE/Silicone. Added features of this material include: Easy Molding. Electrically Conductive, Wear.. |
|||
Linear Mold Shrinkage, Transverse | 0.0050 cm/cm @Time 86400 sec |
0.0050 in/in @Time 24.0 hour |
ASTM D955 |
SABIC Innovative Plastics LNP STAT-KON DX04490 PC LNP* STAT-KON* DX04490 is a compound based on Polycarbonate resin containing Proprietary Filler(s). Added feature of this grade is: Electrically Conductive. |
|||
Linear Mold Shrinkage, Transverse | 0.0050 cm/cm @Time 86400 sec |
0.0050 in/in @Time 24.0 hour |
ISO 294 |
SABIC Innovative Plastics LNP STAT-KON DX04490 PC LNP* STAT-KON* DX04490 is a compound based on Polycarbonate resin containing Proprietary Filler(s). Added feature of this grade is: Electrically Conductive. |
|||
Linear Mold Shrinkage, Transverse | 0.0050 cm/cm @Time 86400 sec |
0.0050 in/in @Time 24.0 hour |
ISO 294 |
SABIC Innovative Plastics LNP STAT-KON SE003 PA 12 LNP* STAT-KON* SE003 is a compound based on Nylon 12 resin containing 15% Carbon Fiber. Added feature of this material is: Electrically Conductive. |
|||
Linear Mold Shrinkage, Transverse | 0.0050 cm/cm @Time 86400 sec |
0.0050 in/in @Time 24.0 hour |
ASTM D955 |
SABIC Innovative Plastics LNP STAT-LOY A3000 ABS LNP STAT-LOY* A3000 is a compound based on ABS resin. Added feature of this material is: Antistatic. |
|||
Linear Mold Shrinkage, Transverse | 0.0050 cm/cm @Time 86400 sec |
0.0050 in/in @Time 24.0 hour |
ASTM D955 |
SABIC Innovative Plastics LNP THERMOCOMP DF002ERH PC LNP THERMOCOMP* DF002ERH is a compound based on Polycarbonate resin containing 10% Glass Fiber. Added features of this material include: Easy Molding, Healthcare, Mold Release. |
|||
Linear Mold Shrinkage, Transverse | 0.0050 cm/cm @Time 86400 sec |
0.0050 in/in @Time 24.0 hour |
ASTM D955 |
SABIC Innovative Plastics LNP THERMOCOMP DF002ERJ PC LNP THERMOCOMP* DF002ERJ is a compound based on Polycarbonate resin containing Glass Fiber. Added features of this material include: Easy Molding, Healthcare. |
|||
Linear Mold Shrinkage, Transverse | 0.0050 - 0.0070 cm/cm @Time 86400 sec |
0.0050 - 0.0070 in/in @Time 24.0 hour |
ASTM D955 |
SABIC Innovative Plastics LNP THERMOCOMP DF003E PC (Asia Pacific) LNP* Thermocomp* DF003E is a compound based on Polycarbonate resin containing Glass Fiber. Added features of this material include: Easy Molding. |
|||
Linear Mold Shrinkage, Transverse | 0.0050 cm/cm @Time 86400 sec |
0.0050 in/in @Time 24.0 hour |
ASTM D955 |
SABIC Innovative Plastics LNP THERMOCOMP DX06409 PC LNP* THERMOCOMP* DX06409 is a compound based on Polycarbonate resin containing 20% Glass Fiber. Added features of this material include: Easy Molding, Mold Release, Healthcare. |
|||
Linear Mold Shrinkage, Transverse | 0.0050 - 0.0060 cm/cm @Time 86400 sec |
0.0050 - 0.0060 in/in @Time 24.0 hour |
ASTM D955 |
SABIC Innovative Plastics LNP THERMOCOMP LC003E PEEK LNP THERMOCOMP* LC003E is a compound based on Polyetheretherketone resin containing 15% Carbon Fiber. Added features of this material include: Easy Molding, Electrically Conductive |
|||
Linear Mold Shrinkage, Transverse | 0.0050 - 0.0070 cm/cm @Time 86400 sec |
0.0050 - 0.0070 in/in @Time 24.0 hour |
ASTM D955 |
SABIC Innovative Plastics LNP THERMOCOMP LF004E PEEK (Asia Pacific) LNP* Thermocomp* LF004E is a compound based on Polyetheretherketone resin containing Glass Fiber. Added features of this material include: Easy Molding. |
|||
Linear Mold Shrinkage, Transverse | 0.0050 cm/cm @Time 86400 sec |
0.0050 in/in @Time 24.0 hour |
ASTM D955 |
SABIC Innovative Plastics LNP THERMOCOMP TH0815A LNP* THERMOCOMP* TH0815A is a compound based on Polyurethane resin containing High Specific Gravity Filler. Added features of this material include: High Specific Gravity. |
|||
Linear Mold Shrinkage, Transverse | 0.0050 cm/cm @Time 86400 sec |
0.0050 in/in @Time 24.0 hour |
ISO 294 |
SABIC Innovative Plastics LNP THERMOCOMP ZFM62P PPE+PS LNP* THERMOCOMP* ZFM62P is a compound based on PPE+PS resin containing 10% Glass Fiber, 30% Mical. Added features of this material include: Exceptional Processing. |
|||
Linear Mold Shrinkage, Transverse | 0.0050 cm/cm @Time 86400 sec |
0.0050 in/in @Time 24.0 hour |
ASTM D955 |
SABIC Innovative Plastics LNP VERTON MX02795 PP (Asia Pacific) LNP* Verton* MX02795 is a compound based on Polypropylene resin containing Long Glass Fiber. Added features of this material include: Chemically Coupled, Heat Stabilized, UV Stabilized. |
|||
Linear Mold Shrinkage, Transverse | 0.0050 cm/cm @Time 86400 sec |
0.0050 in/in @Time 24.0 hour |
ASTM D955 |
SABIC Innovative Plastics LNP STAT-KON DDF029 PC LNP STAT-KON* DDF029 is a compound based on Polycarbonate resin containing Carbon, Glass Fiber. Added features of this material include: Electrically Conductive. Flame Retardant. |
|||
Linear Mold Shrinkage, Transverse | 0.0050 - 0.0070 cm/cm @Time 86400 sec |
0.0050 - 0.0070 in/in @Time 24.0 hour |
ASTM D955 |
SABIC Innovative Plastics LNP STAT-KON DE0049P PC LNP* STAT-KON* DE0049P is a compound based on Polycarbonate resin containing 20% Carbon Fiber. Added features of this material include: Exceptional Processing, Flame Retardant. Electrically Conduct.. |
|||
Linear Mold Shrinkage, Transverse | 0.0050 cm/cm @Time 86400 sec |
0.0050 in/in @Time 24.0 hour |
ASTM D955 |
SABIC Innovative Plastics LNP THERMOCOMP UF009S PPA LNP THERMOCOMP* UF009S is a compound based on Polyphthalamide resin containing 45% Glass Fiber. Added features of this material include: Heat Stabilized. |
|||
Linear Mold Shrinkage, Transverse | 0.0050 cm/cm @Time 86400 sec |
0.0050 in/in @Time 24.0 hour |
ASTM D955 |
SABIC Innovative Plastics LNP VERTON MX02795 PP LNP* VERTON* MX02795 is a compound based on Polypropylene resin containing Proprietary Fillers. Added features of this material include: Heat Stabilized, UV Stabilized, Structural. |
|||
Linear Mold Shrinkage, Transverse | 0.0050 cm/cm @Time 86400 sec |
0.0050 in/in @Time 24.0 hour |
ASTM D955 |
SABIC Innovative Plastics LNP VERTON PV007 PA 6 LNP* VERTON* PV007 is a compound based on Nylon 6 resin containing 35% Long Glass Fiber. Added feature of this grade is: Structural. |
|||
Linear Mold Shrinkage, Transverse | 0.0050 cm/cm @Time 86400 sec |
0.0050 in/in @Time 24.0 hour |
ASTM D 955 |
SABIC Innovative Plastics LNP Verton NV006E PC/ABS LNP* Verton* NV006E is a compound based on PC/ABS resin containing Long Glass Fiber. Added features of this material include: Easy Molding.This data was supplied by SABIC-IP for the Americas region.. |
|||
Linear Mold Shrinkage, Transverse | 0.0050 cm/cm @Time 86400 sec |
0.0050 in/in @Time 24.0 hour |
ASTM D955 |
SABIC Innovative Plastics LNP VERTON PV007 PA 6 (Asia Pacific) LNP* Verton* PV007 is a compound based on Nylon 6 resin containing Long Glass Fiber. |
|||
Linear Mold Shrinkage, Transverse | 0.0050 cm/cm @Time 86400 sec |
0.0050 in/in @Time 24.0 hour |
ASTM D955 |
SABIC Innovative Plastics LNP VERTON UV00AS PPA LNP* VERTON* UV00AS is a compound based on Polyphthalamide resin containing 50% Long Glass Fiber. Added features of this material include: Heat Stabilized, Structural. |
|||
Linear Mold Shrinkage, Transverse | 0.0050 - 0.0070 cm/cm @Time 86400 sec |
0.0050 - 0.0070 in/in @Time 24.0 hour |
ASTM D955 |
SABIC Innovative Plastics LNP STAT-KON ME003S PP LNP* STAT-KON* ME003S is a compound based on Polypropylene resin containing 15% Carbon Fiber. Added features of this material include: Electrically Conductive, Heat Stabilized. |
|||
Linear Mold Shrinkage, Transverse | 0.0050 cm/cm @Time 86400 sec |
0.0050 in/in @Time 24.0 hour |
ASTM D955 |
SABIC Innovative Plastics LNP THERMOCOMP DX06409 PC (Asia Pacific) LNP* Thermocomp* DX06409 is a compound based on Polycarbonate resin containing Glass Fiber. Added features of this material include: Easy Molding, Mold Release. |